A Criterion for the Ductile Fracture of Mild Steel - M. Nagumo 3
A New Method for Fracture Toughness (KIC )- Determination - G. Feddern, E. Macherauch 6
A Study of the COD Concept for Brittle Fracture Initiation - T. Kanazawa, S. Machida, Y. Hagiwara, K. Itoga, H. Tsuchiya 9
Applied Stress and Residual Stress near the Crack Tip of Precracked Specimens - G. Hellwig, E. Macherauch 12
Contribution to the Study of Slow Crack Growth Conditions in Thermomechanically Treated Ultra-high Strength Steels - L. Hyspecka, M. Tvrdy, K. Mazanec 15
Correlation of Brittle Fracture Strength and Chevron Notched Charpy Impact Test Results - S. Kanazawa, K. Minami, K. Miya, S. Sato 18
Dependence of Stress Wave Emission upon Brittle and Ductile Fracture Mechanisms - M. Mirabile, E. Palombi 21
Dynamic Crack Opening Displacement; Effect of Yield Stress; Relation with overall Strain - G. Pluvinage, B. Savage, F. Montariol 24
Dynamic Toughness Measurements by Instrumented Drop Weight Impact Tests - J. C: Radon, A. P. Glover, C. E. Turner 28
Effect of Plate Thickness on Brittle Fracture Initiation and Arresting Characteristics for Very Thick Plates - K. Ikeda 31
Effect of Thickness Variations upon the Plane Stress Fracture Resistance Parameter Kc - A. M. Sullivan, C.N. Freed, J. Stoop 34
Einfluß der Dehngeschwindigkeit auf die an Groß – und Kleinproblem ermittelte Kenngroße der linear-elastischen Bruchmechanik - E. Schmidtmann, H. Scherber 37
Errors Associated with Fracture Mechanics Testing - S.D. ANtolovich, G. R. Chanani 40
Experimental Equipment for Studying Mechanical Properties of Materials under Multiaxial Loading with a Wide Temperature Range - N.V. Novikov, A. A. Lebedeyev, B. I. Kovalchuk, V. P. Lamashevsky 43
Fracture Toughness Characterization of Several Aluminium Alloys in Semibrittle Fracture - J. Eftis, H. Liebowitz, D. L. Jones 46
Fracture under Constrained Deformation - M. W. Taylor, G. Mayer 49
Mechanical Behaviour and Transformation Characteristics of Trip Steels - D. N. Lai, U. Block, V. Weiss 52
Modelluntersuchungen zum Bruchverhalten in ingomogenen Materialen unter statisher Belastung - G. Klein 55
New Test Method Measuring Crack Arrest Properties of Steel - K. Ishikawa, K. Tsuya 58
On the influence of Prestraining on the Fracture Toughness of Structural Steels - A. Kochendorfer 61
Physical Aspect of Plasticity in Linear Fracture Mechanics - G. S. Pisarenko, A. J. Krasowsky, G. N. Nadezhdin 64
Relationship between the Fracture Toughness and the Morphology of the Fracture Surface in Steels Resistant to Atmospheric Corrosion - J. Rittinger, P. Tardy 68
Some Mechanical Properties of Solids Tested under Superposed Hydrostatic Pressures - A. S. Wronski 71
Strain and Stress Distribution in Fully Plastic Notched Bars and the Criterion for Ductile Rupture Initiation - S. A. Mohamed, A.S. Tetelmann 74
Study of Crack Initiation – Arresting Conditions in Plane Plates and Cylindrical Model Vessels - M. Brumovsky, K. Kàlna, S. Stepànek, A. Urban 78
Suggestion of Another Idea of Fracture - T. Sendo 82
The Determination of KIC Values from Measurements of the Critical Crack Tip Opening Displacements at Fracture Initiation - J. N. Robinson, A. S. Tetelman 85
The Effect of Temperature and Loading Rate on the Fracture Toughness of Ti-6Al-4V and 70705 - K.H. Galda, F. Link, D. Munz 89
The Effects of Local Plastic Strain on Crack Propagation - J. Q. Clayton, C. B. Rogers, F. P. Bullen 92
The Measurements of Gc under Dynamic Conditions from Crack Propagation Velocity - G. Gandolfi, M. Mirabile, S. Venzi 95
The Significance of General Yielding Fracture Mechanics in the Brittle Fracture Evalution of Structural Steels - J. M. Diez, G. Frederick 98
The Stresses in the Progress of Crack in Tubolar Specimens - A. Krisch 101
Effects of Large Geometry Changes in Crack Tip on Ductile Fracture - H. Miyamoto, T. Miyoshi 104
A Concept of Combined Micro and Macro Fracture Mechanics to Brittle Fracture - T. Yokobori, A. Kamei, T. Kogawa 107
A Ductile-Fracture Instability Model Based upon reduction of geometrically - Necessary Dislocations - W.W. Gerberich, W. Reuter 110
A Quantitative Model for the Temperature, Strain Rate, and Grain Size Dependence of Fracture Toughness in Low Alloy Steel - S. Ensha, A.S. Tetelmann 113
A refined Theory of Spherical Shell with Cracks - G.C. Sih, H.C. Hagendorf 117
A Rupture Criterion for Ductile Fatigue Crack Advance - P. Neumann 120
A Statistical Theory of Fracture Kinetics of Inhomogeneous Materials - A.N. Orlov, V.A. Petrov, V.I. Vladimirov 123
A Thermally Activated Model for the Plastic Flow and Fracture of Solids - D.D. Cioclov 126
Analysis of Random Cracks and Elliptical Holes - M. Isida 129
Atomic Crack Simulation in Fracture Mechanics - P.O. Gehlen, G.T. Hahn, M.P. Kanninen 132
Bending of an Elasto-Plastic Cracked Plate, Including the Effects of Crack Closure - D.P. Jones, J.L. Swedlow 135
Betrachtungen zur Ausbildung von plastischen Verformungen bei dreiachsigem Spannungszustand - V. Safta 138
Crack Tip Plasticity and Fracture Initiation Criteria - J.R. Rice 141
Cracks in Regions of Complex Geometry. Effects of External Loading, Residual and Temperature Stresses on Initiation of Crack Growth - K. Markstrom 144
Critical Crack Opening Displacement In Low Strength Steels - C.G. Chipperfield, J.F. Knott, R.F. Smith 147
Finite Elements and Fracture - J.H. Argyris, W. Aicher, J. Doltsini, K. Willam 150
Growth of Distributed Cracks under Fatigue Loading - H. Kitagawa, M. Isbida, T. Ohira, M. Kuroda 152
Hole Nucleation by Inclusion Separation in Ductile Fracture - A.S. Argon, J. Im 155
Influence of Grain Boundary Carbide on Brittle Fracture - K. H. Reiff 158
Influence of Non-Singular Stress Terms on Small Scale Yielding at Crack Tips in elastic-plastic Materials - S.G. Larsson, A.P. Carlsson 161
Introduction to the Diffusional Theory of Metal Fatigue - S. Pilecki 164
Kinetic Theory Approach to Fatigue Crack Propagation - T. Yokobori, M. Yoshida 167
Microscopical Mechanisms of Crack Growth - V.I. Vladimirov, V.I. Smirnov 170
On the Validness of Critical Stress-Intensity Factors - H.C. van Elst 173
Post Yield Analysis and Fracture in Notch Tension Pieces - J.G. Sumpter, D.J. Hayes, G.T. Jones, C.E. Turner 177
Rapid Crack Propagation in Strips of Finite Width - P. Nilsson 180
Significance of Stress and Strain Fields around Inclusions with Respect to Fatigue Failure - G. Harkegard 183
Strain Fields Investigation in Connection with Failure Criteria Analysis - R.M. Schneiderovitch, O.A. Levin 186
The effect of High Peak Stresses on Damage Accumulation by Low Peaks - T. Kamata, T. Okada, H. Nakamura 190
Theoretical Calculation of the Griffith Criterion of Fracture in Anisotropic Media to Investigate the Correlation between Crystalline Directions and the Orientation of the Crack Surface - T. Mura, S.C. Lin 193
An Interdisciplinary Approach to Fracture and Fatigue Fracture of Solids - T. Yokobori 195
Bruchvorgänge in Gläsern - P. Kerkhof 207
Fracture in Rocks and Engineering Implications - C. Fairhurst, M.P. Hardy 225
Fracture Phenomena in Composites - A. Kelly 245
Fracture Physics in Comminution - H.R. Rumpf 259
Fracture Theories in Industrial Use of Thermoplastic and Glassfiber Reinforced Plastics - E. Gaube, H.H. Kausch 271
Fundamental Knowledge of Fatigue Fracture - O.C. Grosskreuts 281
Mechanics of Fracture in Polymeric Solids - W.G. Knauss 295
Relations between Microstructure and the Fracture Toughness of Metals - G.T. Hahn, A.R. Rosenfield 309
Some Applications of Fracture Mechanics In Power Engineering - R.W. Nichols 319
Technical Application of Fracture Mechanics to Thin-Walled Structures - H. Kihara, K. Ikeda 331
Testing Methods for Determination of Fracture Toughness of Metals - H. T. Corten 344
Zur experimentellen Lebensdauer-Ermittlung von Konstruìctionselementen mit zufallsartigen Beanspruchungen - E. Gassnsr 355
A Study on Fatigue Damage by the Surface Observation of Electrodeposited Copper Crystals - H. Niyamoto, M. Matsunaga, Y. Hagiuda, N. Chiba 371
An Effect of Prior Austenite Grains on the Fatigue Strength of Martensitic Structure - T. Kunio, M. Shimizu, K. Yamada, S. H. Song 374
Correlation between Fracture Toughness and Stretched Zone Size - D. Broek 377
Correlation between the Fracture Toughness and Material Ductility - V. Weiss, M. Sengupta 380
Crack Propagation Properties in Low Alloy Carbon and Their Microfractographic Analysis - H. Takashima, T. Urashima, Y. Yazaki 383
Crack Size and Grain Size Dependence of the Brittle Fracture Stress - R. W. Armstrong 386
Creep Recovery under Cyclic Plastic Strain - T. Udoguchi, Y. Asada, T. Hiroe 389
Dislocation Processes and Plastic Work in Dependence on Crack Velocity in Ionic Crystals - V. H. Schmidt, G. Zies 392
Effects of Pulsed Electron Beam Heating on the Fracture Resistance of High-Strength Aluminium - L. R. Hettche, S. A. Metz, A. L. Cox 395
Effects of Residual Impurities, Carbide Precipitation, and Carbide Stabilization on the Toughness of Alloy Steels - C. J. McMahon 398
Effects of Structural Changes on Fracture- Mechanic Characteristic Magnitudes - W. Dahl, W.-B. Kretzschmann 401
Ermüdungsrißverlauf und Fraktographie von Ermüdungsbrüchen in Aluminium- und Kupfer-legierungen - S. Kocanda, J. Kozubowski 404
Fracture and Elevated Temperature for Austenitic Steel under Cyclic Creep Loading - T. Kawasaki, M. Horiguchi, J. Shibuya 407
Fracture in Hexagonal Closed Packed Metals, Zinc and Beryllium - M. H. Kamdar 410
Fracture Toughness and Subcritical Crack Growth of Austenitic Manganese Steel - R. I. Stephens, C. P. Saxena, R.C. Rice 413
Influence of Second-Phase Particles on the Low-Temperature Fracture Behaviour of Iron - L. Roesch 416
Interpretation of Fracture Behaviour of a Grinding Wheel Material by a Crack-Body Model - H. Miyamoto, K. Homma 419
Mechanical and Metallurgical Factors Influencing the Assessment of Ductile Fracture Resistance - E. F. Walker, D. Elliot 422
Microstructure and Fracture Toughness of 18 Ni Maraging Steel Weldments - H.-D. Steffens, K. Seiffert 425
Misorientation of Blocks and Crystalline Solids Resistance to Fracture - V. I. Betechtin, A. I. Slutsker, A. I. Petrov, S. A. Ivanov, A. N. Bachtibaev 429
On the Mechanism of Fatigue Crack Advance in Ductile materials - P. Keumann 432
On the Nucleation of Microcracks in Metals under External Loading - J. Krzeminski, M. Sokolowski 435
Solute Effects on Deformation and Fracture of Beta Brass - M. M. Shea, N. S. Stoloff 438
Some Results of Examination of Fractures of Aluminium Cast Alloys, Magnesium Alloyed by Means of Fractography - J. Pirs 441
The Characterization of Fast Fracture and Arrest in Structural Materials - G. T. Hahn, R. G. Hoagland, M. F. Kanninen, A. R. Rosenfield 444
The Fracture of Metals with Voids - Y. Ino, Y. Kawada 447
The Fracture Toughness of Beryllium - R. E. Cooper 450
The Influence of Superplasticity on the Fracture Behaviour of Zinc Based Alloys - N. J. Y. Adams, J. A. Belk, H. G. Munro, P. M. Williams 454
The Transition of the Brittle Fracture at Full Scale Yielding to that at Small Scale Yielding - A. Kochendörfer, H. D. Schulze 457
To the Problem of the Ductile-Cleavage Transition of Fracture - D. Aurich 460
Catalytic dissociation and stress corrosion cracking - P.J. Ficalora, Ya-lung Hu, H. W. Liu 463
Der einfluss der Luftfeuchte auf due spezifische bruchenergie in spiegelglas bei constant gehaltenen klein bruchgeschwindigkeiten - H. Richter 467
Effect of aqueous medium composition at elevated temperatures on fatigue strength of carbon steel - V. G. Azbukin, U.F. Balandin, U.I. Zvezdin, V.V. Potapov, N.N. Tkachenko 472
Effect of crack tip damage on KISCC with 4340 steel - S. Kanazawa, N. Taniguchi 475
Hydrogen-induced sub-critical flaw growth in steels under static and cyclic loading conditions - A. H. Priest, P. McIntyre, C. E. Nicholson 478
Influence of corrosion through tap water on fatigue strength and rate fatigue crack propagation in low carbon steels - J. Kermes, J. Ellinger 481
On the theory of electrochemical stress corrosion cracking - G. P. Cherepanov 484
Stress corrosion cracking of Uranium 10 weight per cent molybdenum alloys in gaseous and aqueous environment - A.M. Nomine, D. Bedere, D. Miannay 487
Stress corrosion of heat resistant materials under hot gases - H. Huff, F. Schreiber 490
The role of the mechanical factor in stress corrosion cracking - Y. Katz 493
A Fractographic Study of Fatigue Crack Propagation - R. Koterazawa 497
An Analysis of the Non-Propagating Fatigue Crack Using the Finite Element Method - K. Ohji, K. Ogura, Y. Ohkubo 499
An Analytic Approach to Low Stress fatigue Crack Growth in Titanium - J.L. Robinson, P.E. Irving, G.J. Beevers 502
Analytical Approach to Notch Size Effects In Fatigue - A. Buch 505