CONCLUSIONS The methodology that has been described for the prediction of ply crack formation in some or all of the 90o plies of a multiple-ply cross-ply laminate subject to combined in-plane biaxial loading, out-of-plane through-thickness loading and bending about two orthogonal axes, and thermal residual stresses, has the following properties: • the analysis is exact within the assumptions made, • the stress-strain relations for a damaged laminate may be obtained by differentiating the Gibbs free energy with respect to the loading parameters, and the form of the stress-strain relations is identical to that for undamaged laminates, • the consideration of ply crack closure conditions leads to the important result that the degradation of the properties of the thermo-elastic constants of the laminate is governed by a single parameter Φ that is dependent only on the axial moduli of the laminate in both the damaged and undamaged states, • the form of the property degradation relations enables the complex expression for the Gibbs free energy of a damaged laminate to be written in a simple form, • the results enable the derivation of a relatively simple criterion for the prediction of the loading and thermal conditions that are energetically favourable for ply cracks to form in some or all of the 90o plies, • the ply crack formation criterion may be used to develop a methodology for the prediction of progressive ply crack formation during loading. REFERENCES 1. Li S, Reid S R & Soden P D, ‘A finite strip analysis of cracked laminates’, Mech. Mater. 18, (1994), 289-311. 2. McCartney L N & Pierse C, ‘Stress transfer mechanics for multiple-ply laminates subject to bending’, NPL Report CMMT(A)55, February 1997. 3. McCartney L N & Pierse C, ‘Stress transfer mechanics for multiple ply laminates for axial loading and bending’, Proc. 11th Int. Conf. on Composite Materials, Gold Coast, Australia, July 14-18, 1997, vol. V, 662-671. 4. Smith P A and Ogin S L, ‘Characterisation and modelling of matrix cracking in a (0/90)2s GFRP laminate loaded in flexure’, Proc. Roy. Soc. Lond. A 456, (2000), 2755 - 2770. 5. Smith P A and Ogin S L, ‘On transverse matrix cracking in cross-ply laminates loaded in simple bending’, Composites Part A, 30, (1999), 1003 - 1008. 6. McCartney L N, ‘Stress transfer mechanics for multiple ply cross-ply laminates subject to bending’, summary in Proceedings of 6th International Conference on the Deformation and Fracture of Composites, Manchester, April 2001, pp. 57-66. Full details to be published. 7. McCartney L N & Byrne M J W, ‘Energy balance method of predicting ply crack formation during bend deformation’, to be published. 8. McCartney L N, ‘Prediction of microcracking in composite materials’, in “FRACTURE: A Topical Encyclopaedia of Current Knowledge Dedicated to Alan Arnold Griffith”, (ed. G.P.Cherepanov), Krieger Publishing Company, Melbourne, USA, 1998, 905-916.
RkJQdWJsaXNoZXIy MjM0NDE=