-1SPECIAL LECTURE ENVIRONMENTALLY ASSISTED FRACTURE BEHAVIOR OF SILICON MICROELEMENTS K. Komai1, K. Minoshima1 and T. Terada2 1Department of Mechanical Engineering, Kyoto University, Kyoto, #606-8501, Japan 2Nomura Research Institute, Ltd., Tokyo, #100-0004, Japan ABSTRACT The influence of notch and water environment on the quasi-static and fatigue fracture behavior was investigated in single crystal silicon microelements. The tests were conducted in smooth and notched microcantilever beam samples. Single-crystal Si microelements deformed elastically until final failure, giving a brittle nature. The maximum fracture strength of a smooth microcantilever specimen reached about 7.7 GPa. However, the fracture strength decreased with an increase in notch depth, even though the notch depth was on the order of nanometer. In laboratory air, no fatigue damage was observed even though the surface was nanoscopically examined by an AFM. However, when the fatigue tests were conducted in pure water, the fatigue lives in water were decreased. Atomic force microscopy was capable of imaging nanoscopic cracks, which caused the failure in water. KEYWORDS Single-crystal silicon, Fracture, Fatigue, Notch, Focused ion beam, Water, Fractography, Atomic force microscopy INTRODUCTION In order to develop a reliable micromachine in a service operation, much care must be taken not only to processing methods, but also to micromechanical evaluation, i.e., mechanical properties of µm-sized microelements including fatigue and wear. For mechanical evaluation, Johansson and Schweitz [1] showed
RkJQdWJsaXNoZXIy MjM0NDE=