ORAL/POSTER REFERENCE: ICF100847OR Evaluation of Stress Intensity Factors of Spot Welded Joints Using Meshless Method Kengo SHIMIZU1, Noboru TOMIOKA2 and Akifumi OKABE3 1Mechanical Engineering major, Graduate school of Nihon University, Tokyo Japan 2,3Department of Mechanical Engineering, College of Science & Technology, Nihon University, Tokyo Japan ABSTRACT It has been required strongly to evaluate fatigue strength of spot welded joint accurately in the stage of designing automobile body structure. There is a evaluation method of fatigue strength based on stress intensity factors K in linear fracture mechanics. We applied Element Free Galerkin Method (EFGM) developed by T. Belytschko et al. to calculating stress intensity factors K of spot welded double cup specimen (is called DC for short) under multiaxial loads, and investigated the accuracy of the solutions. This paper shows that K obtained by using EFGM are appropriate results. KEYWORDS Meshless Method, Fractures, Stress Intensity Factors, Spot Weld INTRODUCTION It has been required strongly to evaluate fatigue strength of spot welded joint accurately in the stage of designing automobile body structure. There is a evaluation method based on stress intensity factors K in linear fracture mechanics. In order to obtain value of K accurately using finite element method (FEM), the detail division of elements on spot welded joint model is essential. In crack growth problem, the rearrangement of nodes and elements around a crack tip is needed through progress of crack. Especially, this rearrangement is the most difficult work in three-dimensional problems. Meshless method, which needs no elements on analytical model, is of great advantage to solving crack growth problem. In this paper, we applied EFGM developed by T. Belytschko et al. [1] to calculating stress intensity factors K of double cup specimen (DC) under multiaxial loads, and investigated the accuracy of the solutions. DC SPOT WELDED JOINT AND ANALYTICAL MODEL The test specimen composed of two cups, called DC shown in Figure 1, is spot-welded at center in the bottom of the cups. Dieter Radaj et al. [2] suggested DC for fatigue strength under multiaxial load. We

RkJQdWJsaXNoZXIy MjM0NDE=