ORAL REFERENCE: 040OR EXPERIMENTAL STUDY ON THE EFFECT OF PLASTIC CONSTRAINT ON DUCTIAL TEARING Qing-fen Li 1, Li Li 1, Shang-lin Yang 1, Ping Long 1, Xiu-ting Han 2 and Hua-qing Cao 2 1 College of Mechanical & Electrical Engineering, Harbin Engineering University Harbin 150001, China 2 Daqing Production and Technology Institute, Daqing 163453, Heilongjiang, China ABSTRACT The effect of plastic constraint on the initiation of ductile tears in four different alloy steels has been experimentally studied by measuring the crack opening displacement and J-integral at initiation in three-point bend specimens with deep and shallow notches in this paper. Experimental results of seven groups of different strength alloy steels show that both ì and Jì values of ductile tear from the shallow crack specimens which have less constraint flow field are significantly higher than deeply notched specimens. Slip-line- field analysis shows that, for shallow crack, the hydrostatic stress is lower than that from standard deeply cracked bend specimen, which develops a high level of crack tip constraint, provides a lower bound estimate of toughness, will ensure an unduly conservative approach when applied to structural defects, especially if initiation values of COD and J-integral are used. KEYWORDS: Ductile tearing, plastic constraint, slip line field, toughness, COD, J-integral INTRODUCTION Crack Opening Displacement (COD) and J-integral concepts of fracture are the accepted methods of estimating the significance of a crack or defect in structural steels. In design practice, the critical value at initiation i and Ji , are normally measured on three-point-bend specimens where the crack depth is approximately half the depth of the beam and the plastic flow is confined to the ligament. Since the plastic flow is constrained, the hydrostatic component of stress in these specimens is high. However, in practice many defects are shallow and the plastic flow associated with them reaches the surface of the component. In this case, the hydrostatic component of stress is smaller and the constraint is lower. As a consequence, the assessment for many shallow defects, the normal method is unduly conservative. Experimental and theoretical study on the effect of the ratio of notch depth to specimen depth (a/w) on i and Ji is therefore necessary. Although many previous work have pointed out that shallow crack specimens give markedly higher values of i and Ji than deeply notched specimens [1-6], someone still doubt the correctness of it. In this paper, we examine the effect of shallow notches on ductile tearing in four Chinese alloy steels.
RkJQdWJsaXNoZXIy MjM0NDE=