TABLE 1. POWERLAW COEFFICIENTS FOR THE FLOWCURVE AT AN ENGINEERING STRAIN RATE OF = 5.7 10 &e +1 S -1 σ ε f n C= C n Strain ≤ 0.2 1020 MPa 0.185 Strain > 0.2 871 MPa 0.087 An overview of the flow-stress, which has been derived with the Bakker correction procedure, has been shown in Figure 4. Increasing flow-stress has been observed for strains smaller than 0.4, for large strain values (> 1.4) the flow-stress decreases at increasing strain rate. Note that for strain values in the necking region (larger than 0.2) the strain rate increases at a constant tensile velocity due to necking. 0 250 500 750 1000 1250 0 0.5 1 1.5 Strain [-] Bakker Flowstress [MPa] engineering strain rates: A = 9.5 E -5 1/s B = 6.2 E -2 1/s C = 5.7 E+1 1/s A C B A Figure 4: Flow-stress according to Bakker derived from experiments CURVE FIT OF FLOW STRESS FOR SEVERAL STRAIN RATES The experimental data has been used to fit a relation between flow-stress, strain, and strain rate. This relation was obtained by modifying the Johnson-Cook [6] relation for varying strain, strain rate, and temperature. We obtained: σ ε ε ε ε ε ε ε f gC M s = + + − = = ⋅ ∗ ∗ − − [ ln ][ ( )ln& ] [ & & & ; & . [ ] 905 127 1 1 21 10 0 0 3 1 Pa] (2) in which &εdenotes the true strain rate, and &ε 0 is a reference value of the strain rate. For strain values varying from 0 to 0.02 a linear flow-stress has been taken, the level can be obtained by substituting the
RkJQdWJsaXNoZXIy MjM0NDE=