ORAL/POSTER REFERENCE: ICF1001032OR FRACTURE AND FATIGUE BEHAVIOR OF TOUGHENED DRA, Al-Be, AND BULK METALLIC GLASS COMPOSITES J.J. Lewandowski, J. Larose and S. Solv’yev Department of Materials Science and Engineering Case Western Reserve University Cleveland, Ohio 44106, USA ABSTRACT The fracture and fatigue behavior of discontinuously reinforced aluminum (DRA) composites, Al-Be composites, and toughened bulk metallic glass systems are presented. Data on the effects of particulate reinforcement additions to an aluminum matrix are presented first and illustrate the decrease in toughness typically observed with reinforcement additions in such systems. The effects of incorporating extrinsic toughening regions on the fracture and fatigue crack growth are subsequently presented and show that both the fracture and fatigue crack growth performance can be improved with such additions. Additional work is presented on the behavior of Al-Be composites produced by powder metallurgy techniques. The fracture and fatigue behavior of the constituents are presented in addition to that of the behavior of the Al-Be composites containing, by volume, 70% Be and 30% Al. The addition of Al to produce the Al-Be composite provides improvements to the toughness and some aspects of the fatigue crack growth behavior in comparison to the monolithic Be. Finally, the effects of the addition of a refractory metal containing toughening phase on the fracture behavior of a bulk amorphous material based on the Zr-Ti-Ni-Cu-Be system is presented KEYWORDS: Discontinuously Reinforced Al (DRA), Ultra-light Al-Be composites, bulk metallic glass/composites. 1. INTRODUCTION There is a continuing need for high performance affordable materials with high specific strength and stiffness. The modified Ashby plot shown in Figure 1 illustrates that composites based on a variety of lightweight materials (e.g. Al, Mg, Ti, Be) provide combinations of high specific stiffness and strength which are attractive to the automotive, aerospace, and electronic packaging communities. Recent reviews have illustrated some of the material sources and balance of properties present in the DRA systems [1-3]. While discontinuous reinforcement additions increase the modulus, Figure 2 [1] illustrates the significant decrease in fracture toughness resulting from such additions. The fatigue crack growth characteristics of DRA (Figure 3 – closed symbols) in comparison to the monolithic matrices (Figure 3 – open symbols) are summarized in Figure 3 [1]. The DRA generally exhibits similar/increased fatigue thresholds and higher Paris Law slopes in comparison to the monolithic matrices upon which they are based [1]. Ultra-light materials based on Be also present some interesting combinations of properties. While Figure 1 illustrates that extra-ordinary combinations of specific stiffness and strength are possible with monolithic
RkJQdWJsaXNoZXIy MjM0NDE=