ICF10B

0 10 20 30 40 0 10 20 30 40 V-notch length (mm) Length of pattern I (mm) 5 3 4 6 2 1 Figure 7: The relationship between the V-notch length and the length of pattern I. The numbers correspond to the run numbers in Table 1. CONCLUSIONS The influence of weld line on the fracture behaviour was investigated by tracing the ripple mark patterns appearing on the fracture surface from double torsion test. One of the patterns indicated that the crack propagated inwardly from the surface of specimen. Although the pattern was assumed to show the effect of V-notch on the weld line surface, the pattern was found to appear even where there was no V-notch on the surface. It can be concluded that V-notch on the weld line surface does not affect the fracture behaviour, while it affects the visual defects of injection moldings.