ICF10C

REFERENCES 1. ASME (1998). ASME Boiler and Pressure Vessel Code, Section VIII, Division 2, ASME, New York. 2. ASME (1998). ASME Boiler and Pressure Vessel Code, Section XI, ASME, New York. 3. BSI (1999). BS 7910, Guide on methods for assessing the acceptability of flaws in fusion welded structures, BSI, London. 4. Czuck, G., Mattheck C., Munz, D. and Stamm, H. Nuclear Engineering and Design, 84, pp. 189-199. 5. Kerezsi, B.B., Kotousov, A.G. and Price, J.W.H. (2000). International Journal of Pressure Vessels and Piping, 77, pp. 425-434. 6. Australian Standards (1995). AS 1548-1995, Steel plates for pressure equipment, Standards Australia, Homebush, NSW. 7. Prater T.A. and Coffin L.F. (1983). In: Corrosion Fatigue: Mechanics, Metallurgy, Electrochemistry and Engineering, ASTM STP 801, pp. 423-444. 8. ASTM (1996) ASTM E 8M-96, Standard test method for tension testing of metallic materials [metric], ASTM, Philadelphia.