results have to be handle with care since the diffusion process is not the same for a spherical powder than for a foil. Indeed, some phases observed for one type of geometry may not exist for the second type. For the Stellite defect a large Tiβ layer is also identified. Moreover, in the small layers close to the defect centre several intermetallics are observed : TiCo, Ti2Co and CoCr. MECHANICAL TESTS In order to analyse the effect of such impurities on the material ductility, tensile tests have been performed at 20K on blocks compacted from voluntarily polluted Ti6Al4V powders. After the compaction cycle, the main pollutions have been localised by X-ray NDE. Smooth and flat tensile specimens have then been machined to settle the impurities in their gage length. A low strain-rate has been imposed in order to avoid thermo-mechanical instabilities likely to occur in this material [1] at that temperature. The main results are displayed in Table 1 showing total elongation in presence of large enough impurities : TABLE 1 TENSILE RESULTS AT 20K : TOTAL ELONGATION FOR EACH POLLUTION pollution no Astroloy In625 Stellite FeNi In718 TE (%) ~15 ~15 ~8 ~5 ~5 ~2 Defect centre Tiβ brittle layer Figure 4: Fracture surface on a In625 pollution at 20K As can be seen in this Table, Astroloy has no dramatic effect on ductility. By contrast, the other defects lead to a strong decrease of total elongation. Stellite, FeNi and In718 are the more dangerous defects. Tensile tests performed at several temperatures up to 293K emphasize the strong temperature influence on the defect/damage interaction : above 50K, no decrease of ductility is observed whatever the impurity present in the Ti6Al4V blocks. A fractography of a specimen tested at 20K and containing a In625 pollution is displayed in Figure 4. Some of the layers observed previously by SEM and TEM examinations (Figures 1 and 2) can clearly be identified in this micrograph : the polyphase centre with a rough aspect and the surrounding Tiβ layer known to be brittle as confirmed on this Figure. The outermost layers exhibit a more classical ductile aspect.

RkJQdWJsaXNoZXIy MjM0NDE=