The configuration of ceramic test nozzles is shown in Figure 3. Two types (Model A and Model B) were designed and were not twisted in considering the easiness of fabrication and analysis. Figure 3: Configurations of turbine nozzle models UNSTEADY THERMAL STRESS ANALYSIS Figure 4 shows the flow chart of the test blade design and unsteady stress analysis procedure. First heat transfer coefficients on the blade surfaces were calculated by a boundary layer approximation method using the specified velocity distribution on the blade surface. Next, the unsteady temperature and stress distributions of the nozzle are analyzed by the MSC/NASTRAN program. In the present study, the target strength of the material at 1,400℃was over 400MPa. Figure 4: Flow chart of the test blade design and unsteady stress analysis procedure