ORAL/POSTER REFERENCE: ICF100861OR Effect of Residual Stress on Fatigue Strength of Steel Modified by WPC Process D. YONEKURA1, H. AKEBONO2, J. KOMOTORI2,M SHIMIZU2 and H. SHIMIZU3 1Dept. of Mech. Eng., The University of Tokushima,2-1 Minami-josanjima-cho, Tokushima, Japan 2Faculty of Science and Technology, Keio University, 3-14-1,Hiyoshi, Kouhoku-ku, Yokohama, Japan 3N.E. LTD., 4-5-12, Sagamidai, Kanagawa, Japan Abstract Rotational bending fatigue tests were carried out on low carbon Cr-Mo steel modified by a combination of Wide Peening Cleaning (WPC) and carburizing, with special attention focused on the effect of surface residual stress on fatigue properties. By combining the carburizing and the WPC process, it is possible to generate a high compressive residual stress near the surface, maintaining a deep layer of compressive residual stress associated with the carburizing. The notched specimens modified by the combined process show significantly higher fatigue strength compared to those modified by single process of carburizing. This is because the extremely high compressive residual stress remained after stress cycling at the surface of the specimens modified by the combined process. Key Words: WPC process, shot peening, fatigue, residual stress, surface modification 1. INTRODUCTION The Wide Peening Cleaning (WPC) process is one of the new surface modifying techniques. The features of the WPC process are as follows: (1) extremely fine and hard particles are used as shot particles and (2) the velocity of shot particles is much higher than that of conventional shot peening methods. The resulting product offers remarkable fatigue resistance relative to that modified by conventional technique. As a consequence, the application of the WPC process to machine parts such as gears and car shafts, has been intensively attempted. However, the reasons for the improvement of fatigue strength have not been well understood.

RkJQdWJsaXNoZXIy MjM0NDE=