Crack growth resistance was measured with a fatigue precracked specimen subjected to increasing crack mouth opening displacement (d) at a fixed rate and using elastic-plastic J-integral fracture mechanics [11]. For cracking in moist air, the plane strain initiation toughness (KJIC ~ KIC [11]) was obtained for specimens with as-processed levels of H and the threshold K (KJTH or KTH) for the onset of H-assisted subcritical cracking was obtained for specimens electrochemically precharged to CH of 100 to 10,000 ppm [3]. For specimens in aqueous chloride solution without H precharging, KTH and stable crack growth rate (da/dt) were measured vs dK/dt [4,6]. RESULTS AND DISCUSSION Fracture Toughness The plane strain fracture toughness of high strength b/a-Ti alloys is deficient compared to martensitic steels at similar high strengths. The data compiled in Figure 2 show that the benefit of the 30% lower density typical of a b-Ti alloy is insufficient to compensate for the very high toughnesses achieved in steels such as AerMet 100 (KIC ~ 120-170 MPaÖm at sYS ~ 1800 MPa). Such steels exhibit up to an order of magnitude higher fracture toughness compared to KIC approaching 25 MPaÖm for very high strength b-Ti alloys. a b Figure 1: Optical (left) and scanning electron (right) micrographs of the deeply etched microstructure of STA Ti-15-3 sheet showing fine a needles precipitated with long axes that intersect to make angles of 0o, 60o and 90o depending on the sectioning plane and consistent with the Burger’s relationship. Tensile Yield Strength (MPa) 800 1200 1600 2000 2400 0 40 80 120 160 200 1 1 2 2 3 3 4 4 4 4 4 4 5 5 Beta-C LCB Ti-15-3 Beta-21S 1 Beta-C 2 Ti-15-3 3 Ti-10-2-3 4 Beta III; Ti-11-3 5 AerMet 100 AF 1410 18Ni Maraging Plane Strain Fracture Toughness (MPa m1/2) Figure 2: The yield strength dependence of plane strain fracture toughness for a variety of high strength b/aTi alloys and martensitic steels fractured in moist air at 25oC.

RkJQdWJsaXNoZXIy MjM0NDE=