ENERGY BALANCE METHOD FOR PREDICTING CRACKING IN CROSS-PLY LAMINATES DURING BEND DEFORMATION L. N. McCartney and M. J. W. Byrne NPL Materials Centre, National Physical Laboratory Queens Road, Teddington, Middlesex, UK, TW11 0LW © Crown Copyright INTRODUCTION Microstructural damage in composite structures arising from the application of mechanical and/or thermal loads is often unavoidable and its effects need to be taken into account when assessing structural performance, especially the occurrence of ply crack formation and delamination. For structures subject to fatigue loading it is desirable to avoid damage occurrence of any kind as it can act as nucleation sites for the growth of macroscopic damage (e.g. delaminations) that eventually leads to the catastrophic failure of the structure. As many structures experience some form of bend deformation during service it is vital that damage formation in the presence of bending is well understood. Of particular relevance to the performance of structures is the prediction of the occurrence of microstructural damage in complex loading modes where out-of-plane bending modes of deformation occur in conjunction with in-plane biaxial and through-thickness loading. While a great deal of research has been devoted to the case of ply cracking in cross-ply laminates subject only to in-plane deformations, the practically important case of out-of-plane bending has received much less attention (e.g. [1-6]). One objective of this paper is to summarise the important results that have been derived using an energy balance method for predicting the conditions for the steady state growth of ply cracks in a cross-ply laminate subject to bending and thermal residual stresses. A second objective is to indicate how the methodology for ply crack formation can be developed without a detailed analysis of the stress transfer that is in fact needed only to estimate the thermoelastic constants of a damaged laminate (as described in [6]). The anti-clastic (i.e. biaxial) bending typical of deformed laminates will be taken into consideration. GEOMETRY AND LOADING CONDITIONS A cross-ply laminate of length 2L, width 2W and total thickness h consisting of perfectly bonded anisotropic layers is considered within a Cartesian coordinate system. The x-direction is taken as the through-thickness direction of the laminate, the y-direction is taken as the axial (longitudinal) direction and the z-direction as the in-plane transverse direction. The bending moments per unit area of loading crosssection for the axial and transverse directions are defined respectively by M 1 2hW x h 2 x,L,z dxdz yy h W W = F HG I KJ zz− σ b g 0 , M hL x h 2 x,y,W dxdy T zz h L L = F HG I KJ zz− 1 2 0 − σ b g . (1) The moments are taken about the mid-plane of the laminate which might not correspond to the neutral axis if the laminate is unsymmetrical and/or damaged in the region of axial tension. The corresponding effective applied axial and transverse stresses are defined respectively by

RkJQdWJsaXNoZXIy MjM0NDE=