ORAL REFERENCE: ENVIRONMENTAL EFFECTS ON FRACTURE AND SUBCRITICAL CRACK GROWTH FOR LIFETIME PREDICTION Tetsuo SHOJI, Junhyun KWON, Qunjia PENG and Guangfu LI Fracture Research Institute, Tohoku University Aoba 01, Aramaki, Aoba-ku, Sendai/980-8579, Japan ABSTRACT In environmentally assisted cracking processes, various parameters in mechanics, chemistry and metallurgy have synergistic effects on fracture and are cross-linked each other. Purely theoretical formulations were developed from slip/oxidation mechanism to deal with the synergy of these parameters for quantitative prediction of crack growth and lifetime of structures in high temperature water environments especially for energy conversion systems The formulations were derived based on an equation of metal oxidation for cracking and analysis of crack tip strain rate for a growing crack in an elastic/plastic work hardening material, in which crack tip strain redistribution due to crack advance was taken into consideration as a crucial part of cracking processes. The obtained formulations were solved numerically to get relations between crack growth rate da/dt and stress intensity factor K in various situation. The well-known phenomena of existence of threshold stress intensities and plateau growth rates in da/dt-K diagrams for many materials/environments combinations can be reproduced by the theoretical formulations from crack tip strain rate point, without any assumption on crack tip water chemistry for the threshold or on diffusion-controlled process for the plateau growth behavior. The effects of crack tip solution chemistry and stress state on the crack growth behavior are discussed in the paper. KEY WORDS: Theoretical prediction, environmentally assisted cracking, stress corrosion cracking, crack growth rate, threshold stress intensity factor, crack tip strain rate, crack tip solution chemistry INTRODUCTION Quantitative evaluation of lifetime of structural components of aged plants and structures is one of the critical issues for safety and reliability evaluation in connection with economics. Such a quantitative capability of life-time prediction needs to be established based on understanding of physical and chemical mechanisms of fracture and sub-critical crack growth where many parameters in mechanics, chemistry and metallurgy have synergistic effects on fracture and are cross-linked each other. In this work, purely theoretical formulations have been developed to deal with the synergy of these parameters for quantitative prediction of crack growth and lifetime of structures in high temperature water environments, especially for energy conversion systems such as light water reactors. Such
RkJQdWJsaXNoZXIy MjM0NDE=