Using this equation, the creep crack growth behaviour was investigated. The law of creep crack growth rate was derived on the basis of a thermal activation process. The law of CCGR for circular notched specimen was different from that for CT specimen and similar as that for creep brittle material, even though material itself is creep ductile. This will be caused by the effect of multi-axial stress field due to a circular notch. Fig. 7: The relationship between CCGR and the Fig. 8: The relationship between CCGR and inverse value of absolute temperature. the initial stress intensity factor. ACKNOWLEDGEMENTS Thanks should be made for financial aid to the Japan Society for Promotion of Science (JSPS) of the RFTF program 97R1201. REFERENCES 1. Yokobori Jr., A.T., Yokobori, T., Sato, K. and Shoji, K.(1985) Fatigue Fract. Eng. Mater.Struct. 8, 4, 315. 2. Nelson, D. V. and Rostami, A. (1997) ASME J. of Pressure Vessel Tech. 119, pp.325-331. 3. Itoh, T., Sakane, M. and Ohnami, M. (1994) ASME J. of Pressure Vessel Tech. 116, pp.90-98. 4. Yokobori, T. (1974) Strength of Mater. 2nd Edition, pp.110-111, Iwanami, Japan. 5. Johnson, H. H. (1965) Mater. Research and Standards, 5, 9, pp.442-445. 6. Schwalbe, K. H. and Hellmann, D. (1981) J. of Testing and Evaluation, 9, 3, pp.218-221. 7. Adachi, T., Yokobori Jr., A. T., Tabuchi, M., Fuji, A. and Yokobori, T. (2001) English J. of Japan Society for Strength and Fracture of Materials, (to be published). 8. Peterson, R. E. (1953) Stress Concentration Design Factors, pp.33-5, John Willy & Sons. 9. JSME (1984) JSME Mechanical Engineers’ Handbook, A. Fundamentals, A4 : Strength of Materials, p.107, JSME, Japan. 10. Yokobori Jr., A. T., Uesugi, T., Yokobori, T., Fuji, A., Kitagawa, M., Yamaya, I., Tabuchi, M. and Yagi, K. (1998) J . of Materials Science, 33, pp.1555-62. 11. Yokobori Jr., A. T. (1997) Advances in Fracture Research, ICF9, 1, pp.39-50. 12. Yokobori Jr., A. T. , Yokobori, T., Tetsuo, N. and Toshiaki, Y.(1992) Mater. at High Temp. 10, 2, pp.108-118.

RkJQdWJsaXNoZXIy MjM0NDE=