ICF100854 OR ESTIMATION OF HIGH CYCLE FATIGUE LIMIT OF HARD SHOT PEENED AUSTENITIC STAINLESS STEEL K. Masaki, Y. Ochi and T. Matsumura Department of Mechanical Engineering and Intelligent Systems, The University of Electro Communications Tokyo, 1-5-1, Chofugaoka, Chofu, Tokyo, 182-8585, Japan ABSTRACT It have been clear that Hard shot-peening (HSP) treatment is very successful for the improvement of the high cycle fatigue strength of austenitic stainless steel. The cause of the improvement is to give the surface hardening layer and compressive residual stress by the treatment, and also the effect of the change of the fracture type from surface crack origin fracture type to subsurface crack origin type. In this study, the fatigue limit at 108 cycles of the HSP treated Type 316L stainless steel was estimated by using the hardness distribution, the HVB (Half Value Breadth) distribution and the residual stress distribution of the specimen. The estimation by using the endurance fatigue limit diagram and the modified Goodman’s diagram was not insufficient method, however. But the fatigue limit by the new estimation using the stress intensity factor was fairly good coincident with the experimental value. KEYWORDS Hard shot-peening, Residual stress distribution, Hardness distribution, Half value breadth, Stress intensity factor, High cycle fatigue strength, Austenitic stainless steel, Fatigue limit estimation INTRODUCTION The surface hardening treatment is a useful method for improving of fatigue properties. And it is also reported by some researchers that how to estimate the fatigue limit of the surface treated materials [1-3]. In generally, the fatigue limit was estimated from the relationship between the applied stress amplitude and the local fatigue limit distribution that was often obtained from fatigue test. However almost methods have been not useful practically because of using the information obtained from the fatigue testing. One of the estimation methods, the suggestion by Murakami et al.[4],using the shot peened spring steel, is well-known because that it is not necessary for the estimation to have fatigue test. But one of the problems of this Murakami’s method is that it needs the assumption in which the position of crack origin is depth range from the surface to 0.4mm [4]. In this study, the estimation method of fatigue limit at 108 cycles using the peening effects and fatigue limit diagram was supposed on the hard shot-peening (HSP) treated Type 316L austenitic stainless steel.
RkJQdWJsaXNoZXIy MjM0NDE=