ICF10B

MATERIAL AND FATIGUE TEST The material used in this study was Type 316L austenitic stainless steel, having the chemical compositions (weight %) of: 0.017 C, 0.39 Mn, 0.014 S, 12.17 Ni, 16.31 Cr and 2.06 Mo. The average of the austenitic structure was about 88µm. The shape and dimensions of specimens are shown in Figure 1. After machining, the center of the specimen was shot-peened using φ0.6mm steel shot with air pressure of 0.196MPa. The Almen intensity was 0.6mmA (hard shot-peening) and the coverage was 100% over. Rotating bending fatigue tests at 50Hz under water-cooling condition by deionized water were carried out. The results of the fatigue tests were shown in Figure 2. The fatigue limit of the HSP treated specimen, about 370MPa, was remarkably improved in comparison with fatigue limit of the n.p. specimen, about 200MPa. ESTIMATION METHOD The fatigue limit was decided by the relation in the local fatigue limit distribution and the applied stress amplitude slope. If the applied stress amplitude slope intersects the calculated local fatigue limit distribution curve, the specimen will be broken. If these two curves do not intersect each other, the specimen will be not broken. And if these two curves intersect in a point, its applied stress amplitude is the fatigue limit of the surface-hardening specimen. Calculation of Local Fatigue Limit Curve In generally, the local fatigue limit σwa can be calculated from the endurance fatigue limit diagram as Eqn.1-a or the modified Goodman’s diagram as Eqn.1-b [5]. Endurance fatigue limit diagram : [MPa] (1-a) ( ) σ =σ σ σ wa w m T −1 Modified Goodman’s diagram : [MPa] (1-b) ) σ =σ σ σ ( wa w m B −1 φ10 φ15 φ20 75 200 50 75 Figure 1: Shape of test specimen (mm) Figure 2: S-N curves under water-cooling condition. 105 106 107 108 109 200 300 400 500 Number of cycles to failure Nf, cycles Stress amplitude σa , MPa SP HSP n.p.

RkJQdWJsaXNoZXIy MjM0NDE=