ORAL REFERENCE: 851 EVALUATION OF BOND PROPERTIES OF CRACK INJECTION REPAIR FOR CONCRETE STRUCTURES M. Kunieda1, T. Kamada1 and K. Rokugo1 1Department of Civil Engineering, Gifu University, Yanagido, Gifu 501-1193, JAPAN ABSTRACT Bond quality is an important factor that affects the performance of repaired members. For crack injection repair, bond strength tests based on Japanese Industrial Standard (JIS) were carried out under conditions that were different from those normally encountered in the field (i.e. the tests involved smaller specimens, smoother surfaces and finer grained materials). Testing methods to evaluate the bond property of repair materials involve a plain concrete as the bulk one. Most repair materials were, however, used in reinforced concrete members. The behavior of repair materials in the members should be also evaluated appropriately. This paper presents the influence of injected surface roughness on the bond properties, in which the bond properties of crack injection materials were evaluated using fracture mechanics parameters. This paper also describes the results of bending tests for reinforced concrete beams repaired by crack injection techniques. The effects of the injected and un-injected parts on the mechanical behavior of repaired reinforced concrete were investigated. KEY WORDS Crack Injection Repair, Bond Property, Surface Roughness, Standard Tests, Flexural Bond Strength INTRODUCTION Good bonding between repair materials and bulk concrete is one of the basic performances required for repaired members. For crack injection repairs, good bonding may increase the stiffness of the repaired members and prevent the penetration of substance (e.g. chloride ions and water). In Japan, the bond property of crack injection materials has been evaluated with the flexural bond strength based on Japanese Industrial Standard (JIS) testing method, where smaller specimens with smooth surfaces for injection are used. This testing method helps to interpret the relative performance of repair materials. However, the evaluated values (indices) obtained from the standard tests depend on the testing methods, such as specimen geometry, loading manner and so on. There is few relation between the evaluated values and the performance of repair materials in existing concrete structures. Regarding the testing method for bond properties in repairs, the location of fracture might be more important (i.e. the fracture of bulk concrete or repair materials, or the delamination of repair materials should be observed). The conventional indices to evaluate the bond property are the tensile bond strength, the flexural bond strength, the shear bond strength and so on. However, it is important to evaluate the bonding after the maximum load in order to estimate the failure process of repaired members. The fracture mechanics parameters, such as tension softening diagrams or fracture energy, were applied to the evaluation of the bond property on construction joint [1,2] and on repair material [3,4].

RkJQdWJsaXNoZXIy MjM0NDE=