performance, the fundamental physical processes of such heat generation at a surface or interface must be clarified and the temperature should be controlled. In order to clarify the origin of heat generation, the source process es, namely the photo-excited carrier dynamics should be studied. For the last 10 years, we have developed new photothermal methods that allow sub-nanosecond time-resolved measurements and offer a nano-scale depth resolution. These methods are Transient reflecting grating (TRG) and Transient reflectivity (TR), and they were applied to various solid surfaces 2,3,4, solid-liquid interfaces 5,6,7,8, multi-layered films 9 and liquid surfaces 10. In this paper, we will show some results obtained by applying the TRG method to thin films and multilayered films of nano-scale thickness. Also, a new type of microscope using the TRG method is proposed for investigating thermal and elastic properties at local places. Futher, the time resolution of the TRG method has been improved from sub-nanosecond to sub-picosecond, and the results are also shown about ultrafast carrier dynamics related to the fundamental processes of thermal generation. Experimental Schematic illustration of the principle for the TRG method is shown in Fig.1. In the TRG technique, two crossed pump pulses are incident at a solid surface and, as a result, the focused spot is irradiated with a pulse of an interference pattern. The complex refractive index at the spot changes due to a physical property change, or grating-patterned surface deformation occurs mainly due to a surface acoustic wave. After the pump pulses irradiation, a probe pulse is also incident there, and the complex refractive index change and the grating-patterned surface deformation are detected through the diffracted light of the probe light. A refractive index change due to photoexcited carriers is observed until several picoseconds, and that due to temperature rise and the following diffusion are observed from several picoseconds to nanoseconds. A surface deformation is detected in the time range of several nanoseconds. Pulsed interference fringes Physical or chemical property change Complex refractive index change Excitation Sample probe pulse Diffracted light ∆n Figure 1 The principle of the transient reflecting grating method. For measurement with a time resolution of sub-nanosecond, Nd-YAG laser ( Pulse width :80 ps, Repetition frequency : 1 kHz, Wavelength : 1064 nm) was used as a light source. The wavelength was frequency-doubled to 532 nm. The pulse was separated into pump and probe pulses using a partial reflective mirror. The pump pulses were further divided into two pulses by a half mirror. The two pump pulses were crossed and irradiated onto the same spot of the sample surface, to coincide in time to form an interference pattern. The probe pulses were also incident at the spot after passing through a computer controlled optical delay line. The diffracted signal of the probe pulses were detected with a photomultiplier, and observed by a computer after averaging the signal with a box-car integrator. In measurements with a time resolution of 200 fs, a regeneratively amplified titanium sapphire laser laser (CPA-1000; Clark-MXR Inc.) was used as a light source. The pulse train wavelength was 800 nm with a repetition rate of 1 kHz and pulse width of 200 fs in full width at half maximum. Only the pump pulses were frequency doubled to a wavelength of 400 nm. The probe pulses remain 800 nm. Results and Discussion
RkJQdWJsaXNoZXIy MjM0NDE=