response of the material. These effects are reflected in the recorded force signal and need to be recognized and properly accounted for if the true impact resistance of the material itself is to be extracted from the experimental data. In a previous work [1] we have demonstrated the usefulness of one-point bending impact experiments (same configuration as in a three-point bending test but without anvils) to elucidate the dynamics of the specimen deformation. Aim of the present work is to extend the investigation to non-standard specimen dimensions in order to elucidate the effects of varying the distribution of the masses involved in the impact process. EXPERIMENTAL DETAILS Impact tests were performed with an instrumented pendulum (Resil 25 by CEAST, Turin) in the Charpy configuration but with the two anvils removed (one-point bending mode). Built-in instrumentation consists of a strain-gauge load cell mounted in the tup of the striker to measure the force acting on its nose and a data acquisition system capable of capturing the force signal every 1 µs. A test speed (load-point displacement rate) of 1 m/s was applied and the impact energies used were far in excess of the energy subtracted by the specimen during the test, so that variations in the striker speed during the test were negligible. Standard (according to 2,3) and non-standard single-edge-notched (SE(B)) specimens of a rigid polyvinylchloride (PVC), were used. The specimen cross-section measured 8.1 mm in thickness (B) and 16.2 mm in width (W), while specimen length (L) and notch depth (a) were varied over wide ranges. The specimens were carefully machined to provide the best possible tup/specimen contact at impact so as to obtain reproducible measurements. An example of the degree of reproducibility generally obtained in this work is shown in Figure 1. 0 100 200 300 0 0.1 0.2 0.3 Load (N) Time (ms) B A Figure 1 - Examples of load-time trace reproducibility: three replicates obtained from specimens with L/W = 4.4, a/W = 0.5. To assess the effect of altering the mass distribution in the specimens, concentrated masses (lead tabs weighing 7.2 g each) were firmly glued either at the two ends of the specimens or at the two sides of the notch on the surface opposite to the impact point, as shown in Figure 2. Figure 2 - Positions of added concentrated masses.

RkJQdWJsaXNoZXIy MjM0NDE=