ICF10B

ICF100543OR EXPERIMENTAL STUDY ON EFFECTS OF MECHANICAL PROPERTIES OF BEAM MATERIALS ON DEFORMATION CAPACITY OF BEAM/COLUMM CONNECTIONS T.NAKAGOMI, K. MATOBA and Y. ICHIKAWA Dept. of Architecture and Civil Engineering, Faculty of Engineering Shinshu University 4-17-1 Wakasato, Nagano-shi, Nagano, Japan ABSTRACT The mechanical property of the beam flange influences the deformation capacity. When yield point, the yield ratio and strain hardening rate are low, deformation capacity of beam to column welded connection excels. 0℃ Charpy absorbed energy of heat affected zone which was the fracture starting point was 130J or more. The Charpy absorbed energy at 0℃ of the beam flange did not influence the deformation capacity. The specimen of the plastic region with a low yield ratio is larger than the specimen with a high yield ratio. Keywords: beam-to-column welded connection, mechanical property, fracture toughness, non-scallop method, deformation capacity 1.Introduction HyogoKen-Nanbu Earthquake in 1995, brittle fracture to accompany beam-ends junction of an architectural iron frame the plastic deformation was confirmed. Absorbed energy (vEo) of 0℃ by the Charpy impact test of the steel material is thought by one of factors which influence brittle fracture at the edge of the beam[1]-[3]. In the SM material (B and C material) and SN materials (B and C material), the lower bound value of vEo is provided for. This research aims the examination of the mechanical property and vEo of the steel material used for the beam of the influence given to the deformation capacity of junction by using the specimen which models the beam-column welded connection. 2.Outline of experiment 2.1 specimen shape and experiment parameter The specimen assumed the shop welding junction type. The size of the beam used six kinds of steel materials of B material of A material of rolling H shape steel RH-400×200×13×21, C 1

RkJQdWJsaXNoZXIy MjM0NDE=