POSTER REFERENCE: ICF10033PR EXPERIMENTAL-NUMERICAL ANALYSIS OF MECHANISMS OF DAMAGE INITIATION IN TOOL STEELS L. Mishnaevsky Jr 1, N. Lippmann 2 and S. Schmauder 1 1 Staatliche Materialprüfungsanstalt (MPA), University of Stuttgart Pfaffenwaldring 32, 70569 Stuttgart, Germany Email: Leon.Mishnaevsky@mpa.uni-stuttgart.de 2 Robert Bosch GmbH, FV/PLM, D-70442 Stuttgart, Germany ABSTRACT SEM in-situ investigations of the micromechanisms of damage initiation and fracture in tool steels are described. The critical state of the material and the damage growth were observed in the tests. It was shown that the initial microcracks in the steels are formed in primary carbides and then join together. A hierarchical finite element model of damage initiation, which included a macroscopic model of the deformation of the specimen under real experimental conditions and a mesomechanical model of damage in real microstructures of steels was developed. Using the hierarchical model, the conditions of local failure in the steels have been obtained. KEYWORDS High speed steels, damage, fracture, micromechanics, microstructure, finite elements, in-situ experiments INTRODUCTION The improvement of service properties of tool steels presents an important source of increasing the efficiency of metalworking industry. In order to develop a numerical model of damage or fracture in the steel, which should serve to predict the lifetime of the steel tool, or to improve the steel properties, one needs to know the mechanisms of damage and fracture in the steels [1-3]. The direct in-situ observation of the fracture mechanisms of the steels under microscope is quite difficult as compared with the case of more ductile materials, since the material fails very quickly. Then, not only qualitative parameters of fracture (like its mechanisms) but also quantitative ones (like critical damage parameters) are of interest. The purpose of this work was to study the mechanisms and conditions of damage initiation and growth in the tool steels both qualitatively and quantitatively. The work includes the 1
RkJQdWJsaXNoZXIy MjM0NDE=