ICF10B

TABLE 2 – CANNON PRESSURE VESSEL FATIGUE LIFE TESTS WITH INITIATION AT THE ID group mean yield inner outer initial stress fatigue degree of strength radius radius crack concentration pressure autofrettage SY; MPa a; mm b; mm ai; mm kt; -- p; MPa n; % 75N 1280 89 187 0.01 1.7 345 0 75A 1020 89 187 0.01 1.7 345 50 55 1230 89 142 0.10 1.0 393 60 20 1120 79 155 0.10 1.0 670 60 between the rifling land and groove. The measured fatigue lives of the sixteen tests from these four groups are shown in Fig. 1, using FIF as the stress parameter in the S-N plot. Referring again to Eqs. 7 and 8, FIF was calculated using: each of the sixteen values of SY ; SY-NOM = 1134 MPa; ai-NOM = 0.10 mm; and values from Table 2. The high correlation of the linear regression expression shows that an FIF based S-N plot gives a good description of fatigue life for cannons, including the significant effect of autofrettage residual stress. 100 1,000 10,000 1,000 10,000 100,000 fatigue life, N; cycles ∆SLOCAL x (SY-NOM/SY) x (ai/ai-NOM) 1/6 - 75A; 50% swage - 75N; 0% swage - 55; 60% swage - 20; 60% swage N = 1.97 x 108 / FIF1.51 R2 = 0.92 Figure 1: Lives for vessels with various % autofrettage MPa Thermal Residual Stress Verified from Thermal Damage Inputs to finite difference calculations of near-bore cannon temperatures are, inevitably, somewhat uncertain. So, before the calculated temperatures are used to determine residual stress, they should be verified by metallographic observations of thermal damage. This has been done for a cannon after the firing of about 40 high temperature rounds [4], see Table 3. About two thirds of the 0.12 mm thickness of chrome showed a transformed microstructure associated with a temperature of about 1320 K. A more certain validation point is TABLE 3 – SUMMARY OF DAMAGE IN A FIRED CANNON thickness of depth of chromium depth of steel depth of crack array; chromium layer damage layer transformation longitudinal section 0.12 mm 0.08 mm 0.19 mm 0.46 mm the well-known 1020 K phase transformation for this type of low alloy Ni-Cr-Mo cannon steel, and metallographs show a consistent, clear depth of 0.19 mm. One further dominant damage feature observed was an ever-present array of constant depth cracks normal to the longitudinal orientation of the cannon, an orientation known to have no significant applied tensile stress. As discussed next, the crack array provides added verification of the calculated depth of thermally induced residual stress due to cannon firing. 0 400 800 1200 1600 2000 0.0 0.1 0.2 0.3 0.4 0.5 distance below bore surface, x ; mm maximim transient temperature, oK transient and residual stress, MPa - observed depths of transformation compressive transient stress tensile residual stress 1320 K; Cr 1020 K; steel transient temperature Figure 2: Firing temperatures and resultant stresses Results of finite difference calculations of temperatures and solid mechanics calculations of transient and residual stresses, using the methods and validation already discussed, are shown in Fig. 2. The solid line shows the calculated maximum temperatures vs distance

RkJQdWJsaXNoZXIy MjM0NDE=