Reference-No.: ICF10059OR FATIGUE BEHAVIOUR OF A SINGLE CRYSTALL NICKEL SUPERALLOY USED IN HEAVY-DUTY GAS TURBINE BLADES WITH FILM COOLING Y. Pan, R. Zimmer, B. Bischoff-Beiermann and D. Goldschmidt Siemens AG Power Generation Group (KWU) Mulheim, Germany ABSTRACT The low cycle fatigue property of a single crystal (SC) superalloy applied in heave-duty gas turbine blades with film cooling holes has been investigated. Special material tests have been carried out for evaluation of the crack behavior. This paper presents results of the testing and appropriate finite element (FE-) calculations. Advantages of SC blades can be revealed and a reliable fatigue life assessment can be achieved with the local approach concept. KEYWORDS Single Crystal Superalloy, High Temperature Low Cycle Fatigue, Heavy-Duty Gas Turbine, Film Cooling Hole, Crack Behaviour, FE-Calculation, Life Assessment INTRODUCTION A new generation of heavy-duty gas turbines with substantially increased output and efficiency has been developed by Siemens [1]. One of the important new technologies applied in this gas turbine, that is well proven in aircraft engines, is the application of single crystal turbine blades with an extensive film cooling. The high temperature mechanical properties of superalloys are strongly dependent on the volume fraction and morphology of γ’-precipitation. In the investigated single crystal superalloy PWA 1483 there is a lower content of grain boundary strengthening elements compared with conventional cast superalloys, [23]. This causes a higher alloy melting point and permits a higher solution heat treatment temperature. Therefore a higher volume fraction of the γ’-precipitation’s with proper morphology can be achieved. This is one of the important reasons for the better mechanical properties of PWA1483 blades. The Laser-Drilling will be widely used in manufacturing of these cooling holes, as a precise hole pattern with exact relative positions can be thereby efficiently produced. However, micro cracks could, especially in a remelt-layer around of the internal hole surface, come into existence. The depth of these cracks must be within the manufacture tolerance.

RkJQdWJsaXNoZXIy MjM0NDE=