Oral Reference: ICF100378OR FATIGUE BEHAVIOUR OF MULTIPHASE STEELS FOR AUTOMOTIVE APPLICATIONS L. Tosal-Martínez, J. Keichel and N. Akdut OCAS N. V., Research center of the SIDMAR Group, ARBED Group Flat Products Division, John Kennedylaan 3, 9060 Zelzate, Belgium nuri.akdut@ocas.be ABSTRACT High strength steels are becoming more and more interesting for the automotive industry as they allow car weight reduction due to lower thickness ensuring the same performance and improved safety by higher energy absorption. A known way of improving the strength, ductility and formability of steels is to make use of additional strengthening and deformation mechanisms by introducing supplementary phases. It is evident that the fatigue behaviour of the materials used for automotive applications is a major point to be taken into account in design and material selection. In this paper the fatigue behaviour of different newly developed high strength multiphase steels (TS>600MPa) including ferritic-bainitic, ferritic-martensitic and TRIP steels is compared with the fatigue behaviour of the commercially available microalloyed steels used at the moment by the automotive producers. Results from laboratory research of pre-strained specimens, which were supposed to be representative for the preceding forming process, will be shown together with results of real components, e.g. wheel disks. Finally, the effect of paint baking on cyclic loading will be evaluated. KEYWORDS Fatigue behaviour, multiphase steels, microalloyed steels INTRODUCTION Car weight reduction has recently become a very important topic for the automotive industry due to the increasing requirements on fuel consumption efficiency that are related to energy savings and environmental restrictions. In this context, a great effort is being done in order to develop new high strength steels that combine both a good formability and a high strength, with the aim of reducing the material thickness of the different automotive parts without resulting in a loss of performance, especially passenger safety. In this paper the fatigue behaviour of some newly developed high strength hot rolled multiphase steels to be used in the automotive sector for, e.g., wheel applications will be presented and compared with the fatigue behaviour of a microalloyed grade that is currently used by the wheel producers. Recently, first industrial wheel production trials have been carried out using those multiphase steels. E.g., it was possible to reduce thickness and thus weight by using a dual-phase grade, which led to a wheel lighter than one made of aluminium [1].
RkJQdWJsaXNoZXIy MjM0NDE=