ORAL REFERENCE: ICF10071OR FATIGUE CRACK GROWTH IN FERROELECTRIC CERAMICS DRIVEN BY CYCLIC ELECTRIC FIELD D.N. Fang, B. Liu and K.C. Hwang Department of Engineering Mechanics Tsinghua University, Beijing 100084, China ABSTRACT In this paper, fatigue crack propagation of the ferroelectric ceramics with initial penetrated cracks under cyclic electric loading is investigated. The experimental results show that there are two distinct fatigue mechanisms. Under low electric loading, the emergence and growth of microcracks is major mechanism, while under a high electric field, the propagation of the macroscopic crack is dominant. It was found in experiments that the crack growth is in company with electric breakdown occurred inside the crack. KEYWORDS Ferroelectric ceramic, Electric Fatigue, Crack propagation, Cyclic loading INTRODUCTION Electric-field-induced fatigue refers to the deterioration of material properties associated with electric cycling. Experiments by Uchino and Furuta [1], Jiang and Cross [2], Cao and Evans [3], Lynch et al. [4], Hill et al. [5], Tai and Kim [6], Zhu et al. [7], Winzer et al. [8], have shown that cracks grow in ferroelectric ceramics under cyclic electric field. The performance of ferroelectric ceramics in smart structures is often hampered by crack propagation in the devices [1]. Does the crack grow by electric breakdown, or by the stress field near the crack tip? Based on the experimental observation and the analysis, the present paper provides both a physical mechanism analysis and a mechanistic explanation. In this paper, different from most work done by others, the propagation of an initial penetrated crack in ferroelectric ceramics instead of the growth of initial surface cracks produced by indentation is studied. Note that the surface crack belongs to a three-dimensional crack and there exists residual stress in the neighborhood of the indentation. The major obstacle in introducing a penetrated crack in the specimen is the brittleness of ferroelectric ceramics. On the other hand, considered that the ferroelectrics usually are used in the low electric loading, the authors try to investigate the fatigue behavior in a more wide loading range. It is more important to study the case of fatigue with low cyclic amplitude ( ). c E E≤

RkJQdWJsaXNoZXIy MjM0NDE=