plasticity induced crack closure, has been identified as the main variable in explaining, fairly reasonably, the variation of the characteristic features of post-overload transients [1-5]. In recent work, the authors [15] concluded that crack closure was able to explain the influence of the stress ratio on the fatigue crack growth rate in 6082-T6 aluminium alloy, in both regimes I and II of crack propagation. Furthermore, for overload conditions, the influence of several load parameters could be correlated with the variation of crack closure. The present work intends to analyse the transient behaviour observed on crack growth rate following block loading and periodic overloads and to clarify if the observed behaviour can also be correlated with the crack closure phenomenon. EXPERIMENTAL DETAILS The material used in this research was an AlMgSi1 (6082) aluminium alloy with T6 heat treatment. The chemical composition (wt.%) of this alloy was 0.7-1.3 Si, 0.6-1.2 Mg, 0.4-1 Mn, 0.5 Fe, 0.25 Cr, 0.2 Zn, 0.1 Cu, 0.1 Ti, 0.05 other. The mechanical properties of the 6082-T6 aluminium alloy were as follows: 300 MPa tensile strength, 245 MPa yield strength and 9% elongation. Fatigue tests were conducted, in agreement with the ASTM E647 standard, using Middle-Tension, M(T), 3 mm thick specimens with 200 mm and 50 mm length and width, respectively. The specimens were obtained in the longitudinal transverse (LT) direction from a laminated plate. The geometry of the M(T) specimen used in this study was presented elsewhere [15]. The notch preparation was made by electricaldischarge machining. After that, the specimen surfaces were polished mechanically. All experiments were performed in a servo-hydraulic, closed-loop mechanical test machine with 100 kN load capacity, interfaced to a computer for machine control and data acquisition. All tests were conducted in air, at room temperature and with a frequency of 20 Hz. The specimens were clamped by hydraulic grips. The crack length was measured using a travelling microscope (30x) with a resolution of 10 µm. Collection of data was initiated after achieving an initial crack length 2a0 of approximately 12 mm. Four different types of simple variable amplitude fatigue loading conditions were applied in this study, as shown schematically in Figure 1. K t (b) K t (a) K t (c) P t (d) 1K∆ n 1K∆ 1K∆ 2K∆ 2K∆ 2K∆ 2P∆ 1P∆ Figure 1: Applied simple variable amplitude loading sequences: (a) single peak overload; (b) Hi-Lo block; (c) Lo-Hi block; (d) periodic single overloads. The single overload and the block loading tests where performed under constant ∆K and stress ratio R conditions, by manually shedding the load with crack growth. The load shedding intervals were chosen so that the maximum ∆K variation was smaller than 2%. The overloads were applied under load control during one cycle by programming the increase in load to the designated overload value. After the change of load, the associated transient crack growth behaviour was carefully observed. All loading conditions were investigated at R=0.05. The periodic overload tests were performed under load control and the

RkJQdWJsaXNoZXIy MjM0NDE=