ORAL REFERENCE: ICF100940OR FATIGUE CRACK INITIATION AND PROPAGATION FROM REINFORCEMENT FIBER ENDS FOR Ti-Alloy MATRIX COMPOSITES Kazumi HIRANO 1, Hiroyuki YOSHIDA 2 and Shinji MIYAKE 2 1 National Institute of Advanced Industrial Science and Technology (AIST) Namiki 1-2, Tsukuba-shi, Ibaraki-ken 305-8564, JAPAN 2 Kobe Materials Testing Laboratory ABSTRACT The partial reinforcement is very useful concept for a wide practical use of continuous fiber reinforced metal matrix composites (MMCs). It follows the reinforcement fiber ends in MMCs components as a necessary consequence. It is therefore very important to examine the influence of reinforcement fiber ends on long-term durability performance for ensuring structural integrity of MMCs components. This paper investigates the fatigue crack initiation and propagation behavior and summarizes the influence of continuous reinforcement fiber ends on low-cycle fatigue behavior for Ti-alloy matrix composite. The reinforcement fiber ends specimen has shorter fatigue lives than those of standard specimen. In particular, the surface fiber ends specimen has shorter fatigue lives as compared with those of inner fiber ends specimen. Cyclic stress-strain and stress-inelastic strain curve measurements indicate a significant difference in the response of these materials depending on the specimen type and strain level. These differences in the response suggest that fatigue crack initiation and propagation mechanisms play different roles in defining fatigue life. KEYWORDS: Ti-alloy Matrix Composites, SP700, Low-cycle Fatigue, Reinforcement Fiber Ends, Fatigue Crack Initiation and Propagation, Fractographic Examinations, Prediction of Fatigue Lives INTRODUCTION Continuous fiber reinforced metal matrix composites (MMCs) have been researched and developed because of light-weight and high temperature capability for the past twenty years and characterized fatigue damage tolerance based on fracture mechanics [1~6]. They have been applied to various high temperature structural components in the field of aeronautics, aerospace and power generation industries. The continuous fiber partially reinforced Ti-alloy matrix composite rotor bladed ring has also been successfully fabricated on the basis of the design requirements [7,8]. It has been widely recognized that the partial reinforcement is very useful concept for a wide practical use. It followed the reinforcement fiber ends in MMCs components as a necessary consequence. It is therefore very important to investigate the influence of these fiber ends on long-term durability performance for ensuring structural integrity of MMCs components. The final goal of this research is to establish not only the materials database but also the design database also included materials testing and evaluation and damage tolerance fatigue design concepts for continuous fiber reinforced Ti-alloy matrix composite (TMCs) rotating parts in aircraft engines, such as impellers, disks, integrally bladed rotors or bladed disks, and bladed rings now primarily fabricated of nickel based super-alloys. This paper investigates the fatigue crack initiation and propagation behavior and summarizes the influence of

RkJQdWJsaXNoZXIy MjM0NDE=