ORAL REFERENCE: ICF100946OR FATIGUE DAMAGE AND COMPRESSIVE RESIDUAL STRENGTH OF A WOVEN PMC SUBJECTED TO CYCLIC HYGROTHERMAL CONDITIONING Michael G. Castelli and John C. Thesken Ohio Aerospace Institute NASA Glenn Research Center Cleveland, OH 44135 USA ABSTRACT An experimental investigation was conducted to characterize the elevated temperature, fully reversed fatigue response of a hygrothermally conditioned carbon fiber reinforced epoxy composite. The material is a 5 harness satin weave in a high temperature epoxy matrix: AS4/PR500. Elastic modulus and residual compressive strength were recorded as a function of fatigue cycle. Unconditioned material is compared to material exposed to 12 khrs of hygrothermal cycle (HC) mission conditioning. Simulating the usage of a gas turbine propulsor component, the HC mission consisted of a 90 minute hold at 121 °C followed by a 22.5hr soak at 30 °C with 85 % nominal relative humidity. Specimens were then machined into a dogbone geometry that was developed and verified for fully reversed fatigue and static compression testing without anti-buckling supports. Fully reversed fatigue data revealed a deterministic stress-life response. The 12 khrs HC conditioned material experienced an 11 % strength degradation when compared to baseline data prior to mechanical fatigue loading. Residual compressive strength measurements were made at specified compressive modulus degradation levels. When correlated with compressive modulus, these strength data showed a clear degradation due to the HC conditioning. Work is underway to characterize material conditioned to 30 khrs. KEYWORDS Fatigue damage, hygrothermal conditioning, compressive properties, composites, residual strength. INTRODUCTION By improving their economy and quality, advances in fully automated composite fabrication techniques have led to wider use of 2-D and 3-D woven polymer matrix composite (PMC) materials in aerospace applications. However, predicting long term fatigue damage progression and durability of PMC materials under prototypical environments remains a challenge. Here, elevated temperatures, ambient moisture levels, and their combined synergistic effects can lead to enhanced degradation rates [1]. These issues are of particular concern for cases where the potential applications are primary/load bearing structures. Compensating for the lack of accurate
RkJQdWJsaXNoZXIy MjM0NDE=