FATIGUE DAMAGE IN UNIDIRECTIONAL COMPOSITE LAMINATES UNDER CONSTANT STRESS AND CONSTANT STRAIN LOADING CONDITIONS: A COMPARATIVE STUDY N. Bonora1, Newaz, G.2 and Gentile, D.1 1DiMSAT – Dept. of Mechanics, Structures and Environment, University of Cassino 03043 Cassino, Italy 2Mechanical Engineering Department, Wayne State University Detroit (MI) -USA ABSTRACT In this paper the approach to understand fatigue performance of composite laminates is reviewed in the light of a strain-based approach as proposed by the authors. Here, starting from the observation that damage in composite laminates is controlled by the effective strain applied during a fatigue cycle, constant stress fatigue is re-discussed. The strain-based approach allows accounting for the large experimental data scatter usually observed in composite laminates tested under cyclic loading and to give the basis for developing a rationale for reliable fatigue design tools. KEYWORDS FATIGUE, COMPOSITE , DAMAGE INTRODUCTION The possibility to understand and predict composite material performance under cycling loading has been deeply investigated in the last decades. In the majority of the published studies, fatigue behavior of composite materials has been approached as for metals. Large experimental effort has been spent in determining the S-N for different laminate configurations, stacking sequences, matrix-fiber choice, and so on. Mainly experimental data reported in the literature have been obtained under constant stress amplitude. Additionally, composite strength after cycling has been also used as a critical parameter to characterize material fatigue performance, Laws and Dvorak [1], Hashin [2-3], Allen et al. [4]. From all these studies, the following common features arise. Firstly, failure is not a unique concept for composite materials. Traditionally, final failure for metals represents the configuration at the end of life for which the imposed loading conditions are no longer sustained and specimen breaking into two or more parts occurs. On the contrary, complete specimen separation in composite laminates may not occur even under extremely severe damaging conditions. Here, failure intended as loss of performance with respect to the application for which the component is designed for, should be used as a more effective screening criterion in material characterization. A large data scatter always characterize the fatigue life under stress controlled conditions. Usually, small variation of the imposed maximum stress results in a very dispersed data at failure lives. The major consequence is the lack of reliability of the fatigue curve
RkJQdWJsaXNoZXIy MjM0NDE=