ICF10B

4. The engineering definition of an initiated crack has been steadily reducing since the mid 19th century from a length of several millimetres, to one millimetre, to 100 microns, to the size of a single grain, to a few microns (and in the event 0,1 microns or less?). 5. A crack of any size demands plasticity (movement of dislocations) to grow and should not require to wait for the establishment of a permanent slip band. 6. The acoustic microscope of late introduced may differentiate between a slip band and a crack. In 1970, K.P. Zachariah assumed that the crack initiation period was zero and that the whole of lifetime was concerned with two phases of propagation namely (i) a short crack propagation phase (the beginnings of Microstructural Fracture Mechanics) and (ii) a longer crack growth phase defined in terms of EPFM. For a starter crack of two microns, the older definitions of “initiation” were dependent on the resolution of currently available microscopes. On top of it, the early growth rate of a crack far removed from various form of microstructural barriers is rapid but decreases on approaching a barriers. In due course, should all obstacles be overcome, a ruling crack can continue its propagation to failure and be described by continuum mechanics. The “initiation” zone is an initially fast but small propagating crack that may either accelerate, decelerate and arrest to acceleration, or decelerate and arrest to give fatigue limit. It will also be recognized why cracks can and do grow below any of the LEFM definitions of a threshold state. In fact, any size of defect or fatigue crack can propagate if the cyclic stress range is highish. 3.1 Construction All structures, in particular welded ones, embrace large defects, ie a > 0.5 mm, together with stress concentration characteristics. Thankfully Tables of Stress Concentration Factors and Stress Intensity Factors exist but always these are in the main applied after a failure incident when the regions of weakness are obvious to all. Fortunately the condition da/dN = 0 for structures may be analyzed from simple LEFM threshold conditions if an initial defect size D can be precisely estimated (which seldom succeeds in large welded structures). The major issues with engineering construction are, as follows: (i) small stress concentration regions being located in large stress concentration zones, eg notches situated at the structure of 3D formulation (ii) 3D in-service loading patterns being random in intensity, in orientation and acting in- and out-ofphase at different occurances in time (iii) critical region for crack initiation not being recognized; note that fatigue cracks do not have to initiate at the worst stress concentration locations In the next century, for that reason more analyses will be demanded for structures holding complex stress concentration, with cracks ranging in size from round about one to a few millimeters. This will be primarily true for those industries that usually have not yet introduced fracture mechanics into their design interpretations. It is certainly probable that many metal construction will be replaced by composite structures which have the aptitude to turn cracks aside from dangerous track. 3.2 Materials Betterments in metals must and will go ahead, in particular in the composites and multiphase substances. It is to be hoped that material scientists and physicists will develop materials with thicker, stronger and more closely packed obstacles to micro-crack propagation. One can anticipate specific materials being designed and developed for specific utilizations, ie hindering the growth of Stage I and/or Stage II fatigue cracks depending on the application. Since it is hoped that more accurate and flexible systems will be discovered to gauge and monitor the propagation of micron and submicron sized cracks (the acoustic microscope can size cracks of a few microns in length-but is miles away from being a mundane implement for industrial use). Multi-failures in electronic devices will help urge these developments. It is awaited that dislocation theory will find a use, acceptable to engineers, in the development of models for determining the growth characteristics of cracks that are of a comparable size to dislocation aggregations. Who can guess – we may ultimately have a new science of Dislocation Fracture Mechanics. Eventually, a note on the scatter of fatigue data. In the next century serious attempts will have to be made to present scatter in a proper perspective probably starting with the influences of different test variables on the

RkJQdWJsaXNoZXIy MjM0NDE=