ICF100509OR Flow and Fracture of Free-Standing Thin Films and Multilayers Haibo Huang, Denis Y.W. Yu and Frans Spaepen Division of Engineering and Applied Sciences, Harvard University, Cambridge, MA 02138, USA ABSTRACT Free-standing polycrystalline films of Ag, Cu and Ag/Cu multilayers were tested in tension using an optical diffraction grating for the measurement of the strain. The yield stress and the rate of work hardening both increase strongly with decreasing layer thickness. These effects combine to raise the stress for ductile fracture up to 700 MPa and to lower the maximum plastic strain. KEYWORDS Thin films, multilayers, yield stress, Hall-Petch, work hardening, fracture stress, ductile fracture. INTRODUCTION The study of the mechanical properties of thin films and multilayers is of considerable technological interest. At the same time, the microstructural control provided by the deposition processes of these films makes it possible to study systematically the effects on mechanical behavior of two length scales, the grain size and the individual layer thickness. These are not independent: if the deposition temperature is sufficiently high to allow extensive surface diffusion, the grain size is similar to the thickness of the film (if single component) or of the individual layer thickness in multilayers [1,2]. The main difficulty in the mechanical testing of thin films is the accurate measurement of the strain, which should be carried out directly on the deforming sample [3,4,5]. In our laboratory, we developed a technique based on optical diffraction from a lithographically

RkJQdWJsaXNoZXIy MjM0NDE=