bilayer repeat length of 40 nm. Although the overall shape of the surface is more planar than that in Figure 4(a), there are many "vein"-like features present that indicate the occurrence of extensive plastic flow. The edges of the pits also indicate that they were formed by local plastic flow. The fracture of the Ag/Cu multilayers is intrinsically ductile. The fracture stress increases with decreasing repeat length due to the increase in, first, the yield stress, and then the rate of work hardening. The decrease in the ductility is directly attributable to work hardening as well. The absence of macroscopic yielding and the lower strength in the multilayers with the shortest repeat lengths is most likely due to the samples being more sensitive to alignment in the apparatus when there is less plastic accommodation. CONCLUSION The interfaces in metallic multilayers can be very effective obstacles to dislocation motion, leading to substantial increases in yield stress as well as in the rate of hardening. These effects combine to raise the resistance to ductile fracture in these materials. ACKNOWLEDGEMENTS We thank Warren MoberlyChan for assistance with the electron microscopy, and Marc Verdier, David Embury, Amit Misra and Harriet Kung for useful discussions. This work was supported by the Harvard Materials Research and Engineering Center under contract DMR-98-09363. HH and DYWY acknowledge support by a predoctoral fellowship from the AlliedSignal Corporation. REFERENCES 1. Thompson, C.V. and Carel, R. (1996) J. Mech. Phys. Solids 44, 657. 2. Verdier, M., Huang, H., Spaepen, F., Embury, J.D., Hawley, M. and Kung, H. unpublished. 3. Read, D.T. (1998) Meas. Sci. Technol. 9, 676. 4. Sharpe, W.N. (1982) Opt. Engineering 21, 483. 5. Kretschmar, A., Kuschke, W.M., Baker, S.P. and Arzt, E. (1997) Mater. Res. Soc. Symp. 436, 59. 6. Ruud, J.A., Josell, D., Spaepen, F. and Greer, A.L. (1993) J. Mat. Res. 8, 112. 7. Huang, H. and Spaepen, F. (2000) Acta mater. 48, 3216. 8. Chokshi, A.H., Rosen, A., Karch, J. and Gleiter, H. (1989) Scripta metall. 23, 1679. 9. Misra, A., Verdier, M., Lu, Y., Kung, H., Mitchell, T.E., Nastasi, M.and Embury, J.D. (1998) Scripta metall. 39, 555. 10. Embury, J.D. and Hirth, J.P. (1994) Acta metall. Mater. 42, 2051.
RkJQdWJsaXNoZXIy MjM0NDE=