ICF10B

ORAL REFERENCE ICF0744 FOREIGN OBJECT DAMAGE AND HIGH-CYCLE FATIGUE THRESHOLDS IN TI-6AL-4V J. O. Peters**, B. L. Boyce, J. M. McNaney and R. O. Ritchie Department of Materials Science and Engineering, University of California, Berkeley, CA 94720-1760 ABSTRACT The objective of this study is to define limiting threshold conditions for high cycle fatigue (HCF) in the presence of foreign object damage (FOD) in an engine Ti-6Al-4V alloy. Impacts in the form of FOD were simulated by firing steel spheres onto tensile fatigue specimens at velocities of 200 to 300 m/s. Such FOD was found to reduce the fatigue strength of the alloy, primarily due (i) stress concentration, (ii) microcrack formation, (iii) impact-induced plasticity and (iv) tensile residual stresses associated with the impact damage. Two groups of fatigue failures could be identified. The first group initiated directly at the impact site, and can be readily described through a Kitagawa-Takahashi approach, where the limiting threshold conditions are defined by the stress-concentration corrected smooth-bar fatigue limit (at microstructurally-small crack sizes) and a “worst-case” fatigue crack growth threshold (at larger “continuum-sized” crack sizes). The second group of failures was caused by fatigue cracks that initiated at locations remote from the impact site in regions of high tensile residual stresses. By evaluating the effect of such residual stresses as a superimposed mean stress, specifically by conducting smooth-bar S-N tests at load ratios between -1 and 0.8, it was found that simple superposition of the applied and initial residual stresses provided a significant contribution to the FOD-induced reduction in fatigue strength by affecting the local load ratio. Such factors are considered in a modified Kitagawa-Takahashi approach to provide a basis for the effect of FOD on HCF failures in Ti-6Al4V. To evaluate the role of surface treatments to enhance high-cycle fatigue resistance, fatigue specimens were also laser shock peened prior to FOD-impact and subsequent fatigue loading. The initial results of these HCF failures of laser shock peened samples are briefly discussed. KEYWORDS Ti-6Al-4V, foreign object damage, high cycle fatigue, residual stress, fatigue crack initiation, fatigue crack growth threshold INTRODUCTION High-cycle fatigue (HCF) of turbine engine disk and blade components represents one of the major concerns limiting with the readiness and safety of military aircraft. Since in-flight HCF conditions invariably involve high cyclic frequencies, small crack sizes and (depending on blade location) very high mean stress levels, a preferred approach for design against HCF can be considered in terms of the concept of a threshold for no fatigue crack growth [1-3]. Foreign object damage (FOD) by small hard particles has been identified as a key factor associated with such HCF related failures in titanium alloy blades [1,2]. Specifically, FOD has been found to reduce the fatigue strength of fan and compressor blades, principally by causing stress-raising notches and microcracks [2] at impact sites; this, in association with the plastic deformation and tensile residual stresses resulting from such impacts [1], can lead to the early nucleation and growth of fatigue cracks. ** Now with the Department of Physical Metallurgy and Materials Technology, Technical University Hamburg-Hamburg, 21071 Hamburg, Germany

RkJQdWJsaXNoZXIy MjM0NDE=