A low alloy steel (JIS SNCM439: 0.40C, 0.22Si, 0.78Mn, 0.02P, 0.013S, 0.18Cu, 1.78Ni, 0.83Cr, 0.2Mo, in mass%, 1123K x 1h gas cooled, 1123K x 1h oil cooled and 433K x 1h gas cooled) and a bearing steel (JIS SUJ2: 1.01C, 0.23Si, 0.36Mn, 0.01P, 0.007S, 0.06Cu, 0.04Ni, 1.45Cr, 0.02Mo, in mass%, 8ppmO, 1108K x 40min oil(353K) cooled, 453K x 2h air cooled) were investigated. The notch parts of specimen shown in Fig.1 were finally finished by 100 mesh grindstone, 1500 mesh emery paper and shot-peening treatments shown in Table 1, respectively. Cantilever type rotating bending fatigue tests have been carried out in laboratory air at room temperature. RESULTSAND DISCUSSION Effects of surface treatment on fatigue strength Figures 2 (a) shows the effects of surface treatment on fatigue strength in a low alloy steel, JIS SNCM439. High stress amplitude loading for rough surface finish promotes surface cracking. The influence of surface treatments on the fatigue life under same stress amplitude is large in short life region. Low stress amplitude loading for all surface treatments promote fish-eye type cracking. The influence of surface treatments on the fatigue limit is hardly admitted in long life region. Figure 2 (b) shows the results of a bearing steel, JIS SUJ2. Most of the specimens finished by 100 mesh grindstone were surface cracking, and the fatigue life under the same stress amplitude has changed a little depending on the processing lot. Fine finish by 1500 mesh emery paper and surface treatments by shot-peening promote fish-eye type, subsurface cracking. Two open circle symbol data with * marking for the specimens polished by 1500 mesh emery paper show the surface cracking, which the cracking start from the inclusion located on the notch surface. There is a tendency to which the fatigue limit decreases in the range that fatigue life exceeds 107 cycles, and the tendency is remarkable in the bearing steel. The fatigue life varies remarkably for the 100 mesh grinding finish, because of the grinding processing damage. 2
RkJQdWJsaXNoZXIy MjM0NDE=