ICF10B

Internal electrodes are largely adopted in electronic and electromechanical devices made from piezoelectric ceramics. These embedded electrodes may naturally function as pre-conductive cracks or notches, which may lead to failure of these devices under combined electric and mechanical loads. However, only few experimental observations of conductive cracks in piezoelectric ceramics have been reported so far. Lynch et al. [2] carried out indentation fracture tests on electroded surfaces submerged in electrically conducting NaCl solution and in distilled water. In both cases, tree-like damage grew from the indented electrode under the cyclic electric field. Heyer et al. [3] studied the electromechanical fracture toughness of conductive cracks in PZT-PIC ceramics. They conducted four-point bending tests on pre-notched bars, in which the poling direction was toward the jig surface and the notch was filled with NaCl solution to make the crack conducting. Wide scattering results were obtained under a large applied electric field ( 1/2 / 50 K kv m E > 1/ 2 / m , where is the applied electric intensity factor). The critical stress intensity factor increased as the applied intensity factor of the electric field strength changed from 30 to . When the applied electric intensity factor was relative small, within the range of − to 15 , they could explain the experimental data using a domain-switching-based model. Fu et al. [4] conducted fracture tests of conductive cracks in poled PZT-4 ceramics, in which only positive electric field was applied. They found that under purely electric loading, there existed a critical energy release rate that was named the electric fracture toughness. The electric fracture toughness is a material property, similar to the mechanical fracture toughness. Furthermore, the electric fracture toughness under positive electric loading is about 25 times higher than the mechanical fracture toughness [4]. The present work studies the fracture behavior of conductive cracks in poled PZT-4 ceramics under negative electric fields and combined electric and mechanical loads as well. EK 1/ 2 / kv m 15 1/ 2 / 90kv m − 1/ 2 / m kv kv EXPERIMENTAL PROCEDURE The material used in this study was poled lead zirconate titanate ceramics (PZT-4, Morgan Matroc). Prenotched or cracked compact samples were adopted in the fracture tests under purely mechanical, purely electric and mixed mechanical and electric loads. All samples had the width w=10mm, height h=10mm and thickness t=3mm. A pre-notch or crack was cut in each sample with a 0.15mm thick diamond saw parallel to the poling direction, and further sharpened by a 0.12 mm diameter wire saw. After the cutting, the samples were cleaned ultrasonically in distilled water for 20 seconds. For conductive cracks, silver paint was filled into the notch (crack) to make it function as an electrode. Figure1 schematically shows the sample geometry and loading. The following three types of tests were conducted. 1) Purely mechanical loading (PM). On purpose, the ligament, l, varied from sample to sample and ranged from 2.5 to 4.5 mm. The tests were conducted on a mechanical testing machine (Miniature Materials Tester, Polymer Laboratories) at a crosshead rate 0.1mm/min under uniaxial tension. 2) Purely electric loading (PV). A static voltage was applied to a sample and manually increased until the sample was failed. Positive and negative electric fields, which were respectively parallel and anti-parallel to the poling direction, were applied in the tests. 3) P V poling directionn conductive w P l Fig.1 Depiction of the sample geometry and loading.

RkJQdWJsaXNoZXIy MjM0NDE=