DISCUSSION First we consider the behavior in the center region of the specimen. The value Γ0 = 11.5 kJ/m2 yields the correct fracture initiation behavior; also the first stages of crack extension are predicted well. With increasing vLL, the crack extension becomes much too high. Γ0 = 17.5 kJ/m2 clearly underestimates the crack growth for small vLL; however, at large vLL, the crack growth rate is still overestimated. It can be concluded that it will be impossible to find any pair of constant Γ0 (M) and Tmax (M) values so that the model reflects the experimental behavior. Either Γ0 (M) or Tmax (M) or both must increase during the crack extension, at least, for the initial stages of crack growth. This could be due to the loss of constraint with increasing deformation [21]. The question, whether a crack growth region of constant cohesive parameters will appear after the initial transition region as it was observed in [8,9], cannot be decided yet. Directly at the side surface, even a value of Γ0 = 17.5 kJ/m2 leads to a retarded crack extension for small v LL. The reason might be that a too large value of the cohesive strength was taken (Tmax = 1100 MPa, instead of the “correct” value for plane stress, Tmax (pl σ) ≈ 800 MPa). For large v LL-values, Γ0 = 17.5 kJ/m2 overestimates ∆a, Γ0 = 24 kJ/m2 slightly underestimates ∆a. It should be noted however, that the experimental determination of ∆a is difficult and that the scatter of the data is large. As a summary we can state that a comparison between the experimental data and the numerical simulation reveals that the parameters of the cohesive zone model depend on the location at the crack front and change during (the first stages of) crack extension. ACKNOWLEDGEMENTS The authors acknowledge gratefully the help of Professor W. Brocks of the GKSS Forschungszentrum Geesthacht, Germany, and the financial support of this work by the Materials Center Leoben under the project number SP7 and by the Österreichische Nationalbank under the project number 7744. REFERENCES 1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 16 17 18 19 20 21 Needleman, A. (1987) J. Applied Mechanics 54, 525. Stüwe, H.P. (1981) In: Three.Dimensional Constitutive Relations and Ductile Fracture, NematNasser, S. (Ed.). North-Holland, 213. Broberg, K.B. (1995) Engng Fracture Mech. 50, 157. Ortiz, M. and Pandolfi, A. (1999) Int. J. Numer. Mech. Engng. 44, 1267. de-Andres, A., Perez, J.L. and Ortiz, M. (1999) Int. J. Solids Struct. 36, 2231. Tvergaard, V. and Hutchinson, J.W. (1996) Int. J. Solids Struct. 33, 3297. Varias, A.G. (1998) Comput. Mech. 21, 316. Siegmund, T. and Brocks, W. (1999) Int. J. Fracture 99, 97. Siegmund, T. and Brocks, W. (2000) ASTM STP 1360, 139. Siegmund, T. and Brocks, W. (2000) Engng Fracture Mech. 67, 139. Kolednik, O. and Stüwe, H.P. (1986) Engng Fracture Mech. 24, 277. Yan, W.-Y., Shan, G.X., Kolednik, O. and Fischer, F.D. (1998) Key Engineering Materials 145-149, 179. Scheider, I. (2001) Bruchmechanische Bewertung von Laserschweißverbindungen durch numerische Simulation mit dem Kohäsivzonenmodell. Dissertation, Technical University Harburg, Germany. ABAQUS, Version 5.7, Hibbit, Karlson & Sorenson Inc. Pawtucket, RI, USA. Scheider, I. (2000) Internal Technical Paper GKSS/WMS/00/19. GKSS Forschungszentrum Geesthacht, Germany. Shan, G.X., Kolednik, O., Fischer, F.D. and Stüwe, H.P. (1993) Engng Fracture Mech. 45, 99. Kolednik, O., Shan, G.X. and Fischer, F.D. (1997) ASTM STP 1296, 126. Kolednik, O. and Stüwe, H.P. (1985) Engng Fracture Mech. 21, 145. Stampfl, J., Scherer, S., Berchthaler, M., Gruber, M. and Kolednik, O. (1996) Int. J. Fracture 78, 35. Scherer, S. and Kolednik, O. (2001) Microscopy and Analysis 70, in press. O’Dowd, N. and Shih, C.F. (1991) J. Mech. Phys. Solids 39, 898.
RkJQdWJsaXNoZXIy MjM0NDE=