ICF10B

coefficient can be determined by inverse analysis [8]. Then time-dependent moisture distributions can be numerically predicted. The moisture profiles in normal concrete can be realistically predicted by the general diffusion equation [9]. In the case of high strength concrete a sink term has to be added to the diffusion equation because of the endogenous drying. If we compare the moisture profile after 7 days of drying for instance the drying process affects the surface near zone in normal concrete only. In high strength concrete endogenous drying, however, leads to an equilibrium hygral potential of 0,8 in the center of drying elements. This effect has a series of consequences with respect to crack formation. From shrinkage tests infinitesimal shrinkage i.e. shrinkage of an infinitesimal thin layer can be obtained by inverse analysis [10]. Crack formation in reinforced beams made of normal and high strength concrete has been simulated numerically. The entering material properties such as elastic modulus, tensile strength and strain softening, hygral diffusion coefficient, coefficient of hygral dilatation have all been determined experimenteally. 5. CONCLUSIONS The following conclusions can be drawn from the results presented in this contribution: - Crack formation and fracture energy depend on the mechanical interaction between inclusions (gravel or crushed stone) and the cement-based matrix. - High strength means generally low ductility and increased risk for crack formation. - A numerical model (numerical concrete) can be used to optimise composite materials such as concrete with respect to well-defined requirements: strength, ductility, durability etc. - Endogenous shrinkage takes place in high strength concrete. This process creates stress states and internal damage which are not covered adequately by most codes so far. REFERENCES 1. A. Hillerborg, M. Modéer and P.E. Petersson, Analysis of crack formation and crack growth in concrete by means of fracture mechanics and finite elements, Cement and Concrete Research, 6, 773782 (1976) 2. F.H. Wittmann, editor, Fracture Mechanics of Concrete Structures, Proc. Second Int. Conf. On Fracture Mechanics of Concrete Structures, Aedificatio Publishers, D-Freiburg (1995) 3. H. Mihashi and K. Rokugo, editors, Fracture Mechanics of Concrete Structures, Proc. Third Int. Conf. Of Fracture Mechanics of Concrete Structures, Aedificatio Publishers, D-Freiburg (1998) 4. F.H. Wittmann, editor, High Performance of Cement-Based Materials, WTA report series No. 15, Aedificatio Publishers (1997) 5. B. Trunk and F.H. Wittmann, Experimental investigation into the size dependence of fracture mechanics parameters, in Ref. 3, pp. 1937-1948 (1998) 6. P.E. Roelfstra, H. Sadouki and F.H. Wittmann, Le béton numerique, Materials and Structures 18, 327335 (1985) 7. E. Brühwiler and F.H. Wittmann, The Wedge splitting test, a new method of performing stable fracture mechanics tests, Eng. Fracture Mechanics 35, 117-125 (1990) 8. X.H. Wittmann, H. Sadouki and F.H. Wittmann, Numerical evaluation of drying test data, Transaction, 10th Conf. On Struct. Mech. In Reactor Technology (SmiRT-10), Vol Q, pp. 71-79 (1983) 9. A.M. Alvaredo, Drying shrinkage and crack formation, Building Materials Reports No. 5, Aedificatio Publishers (1994) 10. G. Martinola, Rissbildung und Ablösung zementgebundener Beschichtungen auf Beton, Building Materials Reports No. 12, Aedificatio Publishers (2000)

RkJQdWJsaXNoZXIy MjM0NDE=