ICF10B

All tests were executed on an INSTRON universal testing machine. The load-line displacement was measured by means of a laser scanner system. The laser double scanner used is favoured for the experimental fracture mechanics examination and works in transmission mode with two parallel laser beams. With these two beams the load-line displacement and crack mouth opening displacement can determined by contactless measurements for the shown specimens (fig. 1) [3]. RESULTS AND DISCUSSION Unfilled and unmodified epoxy resins are brittle and exhibit unstable crack propagation. The estimation of fracture mechanics parameters (stress intensity factor K and J-Integral) by using miniature specimens bases on the analysis of the crack resistance behaviour under quasi-static loading. Toughness values of epoxy resin depend on specimen thickness. Because the experimental estimation of the minimum thickness Bmin is very expensive due to the required great number of specimens, of alternative geometry criteria should be used. The empirical geometry criterion (Eq.1) is valid and independent of loading conditions and the nature of materials failure. 2 min       = Y Ic K B σ β ( 1) The geometry factor β depends on material and on the loading conditions, but it is often considered to be constant. In case of double-logarithmic plotting of β in dependence on the stress-intensity factor K the value β decrease with increasing toughness independent on the used standard or testing protocol. The experimentally obtained fracture mechanics values will be geometry-independent, if it fulfil this geometry criterion of minimal specimen thickness Bmin. With increasing thickness of mini-compacttension specimen geometry independent fracture mechanics values can be found for the epoxy resins. The critical minimum specimen thickness was determined to be 4 mm (fig. 2-filled symbols).Thereby, the fracture mechanics parameters can express the influence of material structure, loading rate, and the test temperature on the toughness by using (CT-) specimens. 1000 100 10 1 0.1 10 100 1000 Thickness 1 mm 2 mm 4 mm 6 mm 8 mm 10 mm KIc [MPamm1/2] β Figure 2: Requirements on specimen geometry for the determination of critical fracture toughness values KIc with miniature specimens Under the view of practice, the fixing of employment limits for epoxies is of a special significance and requires the description of the mechanical properties in dependence on temperature. Up to a tempera-

RkJQdWJsaXNoZXIy MjM0NDE=