ICF10B

ICF100139OR FRACTURE MECHANISMS IN B2 NiTi SHAPE MEMORY ALLOYS Nancy Yang1, Ken Gall2, Huseyin Sehitoglu3, and Yuriy Chumlyakov4 1Materials & Engineering Sciences Center, Sandia National Laboratories, Livermore, CA, 94550 USA 2Department of Mechanical Engineering, University of Colorado, Boulder, CO, 80309 USA 3Department of Mechanical and Industrial Engineering, University of Illinois at UrbanaChampaign, Urbana, IL, 61801 USA 4Tomsk University, 634050 Tomsk, Russia ABSTRACT The fracture mechanisms in single crystal Ti-50.8at%Ni shape memory alloys containing Ti3Ni4 precipitates are studied using the scanning electron microscope (SEM). Aged materials with three different precipitate sizes (50 nm, 150 nm, and 400 nm), which have interfaces ranging from semi-coherent to incoherent, are considered. The primary mechanisms of material fracture identified in the single crystal NiTi are: (1) Nucleation, growth, and coalescence of voids from the Ti3Ni4 precipitates and (2) Cleavage fracture on {100} crystallographic planes. Cleavage fracture and ductile tearing are found to act in conjunction, and the relative dominance of one over the other depends on the local precipitate size. When the Ti3Ni4 precipitates are small and coherent they facilitate mechanism 2. As the Ti3Ni4 precipitate size increases to about 400 nm, the overall fracture is dominated by failure mechanism 1, and the cleavage markings become diffuse. KEYWORDS NiTi, Single Crystals, Cleavage Fracture, Ductile Tearing. INTRODUCTION As evident in a recent review on shape memory alloys [1], the general thermo-mechanical response of NiTi is well characterized for various testing conditions. However, the utilization of NiTi shape memory alloys in long life components requires a thorough understanding of the dominant mechanisms controlling their fatigue and fracture. Under cyclic loading conditions, the failure of NiTi shape memory alloys in service can be caused by either an inability of the alloy to provide the required material response (recoverable displacement or force) or the fracture of the material. Minimal work [2] has been performed on the resistance of NiTi alloys

RkJQdWJsaXNoZXIy MjM0NDE=