ACKNOWLEDGMENTS The research of K. Gall and H. Sehitoglu is supported by a grant from the Department of Energy, Basic Energy Sciences Division, Germantown, Maryland, DOE DEFG02-93ER14393. The research of N. Yang is funded by the Department of Energy. The work of Y. Chumlyakov is supported by grants from the Russian Fund for Basic Researches, grant # 02-95-00350, MOPO (MGTU, Moscow) and from fund 99-03-32579a. REFERENCES [1] Otsuka, K and Wayman, C. M. (1998) Shape Memory Materials, Cambridge University Press, New York, NY. [2] Melton, K. N. and Mercier, O. (1979) Acta. Metall., 27, 137. [3] Chang, K.-M., Darolia, R., and Lipsitt, H. A. (1992) Acta. Metall. Mater., 40, 2727. [4] Hahn, G. T. and Rosenfield, A. R. (1975) Metall. Trans., 6A, 653. [5] Bhattacharya, K. and Kohn, R. V. (1996) Acta Mater., 44, 529. [6] Shu, Y. C. and Bhattacharya, K. (1998) Acta Mater., 46, 5457. [7] Gall, K., Sehitoglu, H., Chumlyakov, Y. I., and Kireeva, I. V. (1999) Acta Mater., 47, 1203.