ICF100404OR FRACTURE OF PIEZOELECTRIC MATERIALS Tong-Yi Zhang* and Minghao Zhao Department of Mechanical Engineering, Hong Kong University of Science and Technology Clear Water Bay, Kowloon, Hong Kong, China, * E-mail: mezhangt@ust.hk ABSTRACT The present work studies, theoretically and experimentally, the fracture behavior of piezoelectric ceramics. For an electrically insulating crack, the ratio of β α/ plays an important role in the energy release rate, where α is the ratio of the minor semi-axis, b, to the major semi-axis, a, of the ellipse, and β is the ratio of the dielectric constant of the cavity to the effective dielectric constant of the material. There are three limiting values in the energy release rate, respectively corresponding to / 0→β α for an electrically permeable crack, →β α/ a finite nonzero value for general cases and →∞ β α/ for an electrically impermeable crack. For an electrically conductive crack, the applied electric field parallel to the crack drives the crack to propagate. When electric yield occurs at a crack tip, the global energy release rate is the same as that derived from linear fracture mechanics, while the local energy release rate shows a linear relationship between the fracture toughness and the applied electric field. The experimental results illustrate that for PZT-841 and PZT-4 ceramics, the degree of scattering of measured data was considerably enhanced by an applied electric field. Either a positive or a negative electric field reduced the fracture toughness. The experimental results also confirmed that there exist mechanical- and electrical-fracture toughness for PZT-4 ceramics and both are material properties. The mechanically- and electrically- critical energy release rates are, respectively, 8.7(±1.1) and 223.7(±45.5) N/m. KEYWORDS piezoelectric medium, crack, energy release rate, fracture toughness, polarization saturation INTRODUCTION Along with the application of piezoelectric materials in more and more sophisticated structures, their mechanical reliability becomes increasingly important. Thus, many efforts have being made to study the fracture behavior of those materials [1-23]. One of the most interesting aspects is about the effect of electric field on the fracture behavior. Many experimental results are inconsistent or even contradicted, which makes the study of fracture of piezoelectric ceramics more challenging. The present work briefly summarizes the work done at the Hong Kong University of Science and Technology, on this topic. TWO-DIMENSIONAL SOLUTION Figure 1 shows schematically a crack of length 2a in an infinite piezoelectric medium under remotely

RkJQdWJsaXNoZXIy MjM0NDE=