ICF1001056OR FRACTURE OF THERMAL SPRAYED NANOSTRUCTURED COATINGS Maurice Gell, Leon Shaw, Eric Jordan, Hong Luo and Daniel Goberman School of Engineering, University of Connecticut Storrs, CT 06269, USA ABSTRACT A nanostructured alumina-13 weight percent titania plasma sprayed coating has been developed with outstanding wear, toughness, adhesion and machinability properties. The optimized properties are associated with a bi-modal microstructure that consists of a fully melted region and a partially melted region. In contrast, a baseline, commercial Metco 130 coating of the same composition contains only the single-phase splat microstructure. The crack growth resistance or “toughness” of each of these materials was investigated using the cracks generated around Vicker’s hardness indents. In Metco 130, long, wide cracks initiate in and propagate along splat boundaries. In the nanostructured alumina-titania, the spherical particles in the bi-modal microstructure serve to trap and deflect the splat boundary cracks. This produces the approximately 100% improvement in the crack growth resistance of the nanostructured coating with the bi-modal microstructure. The volume fraction of the partially melted regions can be systematically varied by changing the plasma flame temperature. It was found that the crack growth resistance of the nanostructured coatings was optimized when the microstructure contains 15-20% of the partially melted spherical particles. KEYWORDS Nanostructured coating, wear resistant coating, plasma sprayed coating, toughness, crack growth resistance. INTRODUCTION A nanostructured alumina-13 w/o titania plasma sprayed coating has been developed that has superior wear resistance, toughness, adhesion and machinability properties [1]. The composition, powder preparation procedure, plasma spray processing parameters, microstructure and properties have been described previously [1-4]. The technology for

RkJQdWJsaXNoZXIy MjM0NDE=