ORAL REFERENCE : ICF100101OR FRACTURE PROCESS OF PM Ti6Al4V AT 20K IN PRESENCE OF IMPURITIES L. Briottet1, N. Scheer1 and D. Guichard2 1 CEA/Grenoble, DRT/DTEN, 17 rue des martyrs, 38054 Grenoble cedex 9, France 2 SNECMA/Division Moteurs Fusée, Forêt de Vernon, BP802, 27208 cedex Vernon, France ABSTRACT PM Ti6Al4V is foreseen to manufacture rocket engine components with complex geometry. The major drawback related to this process is the potential presence of impurities mixed with the initial powder. At cryogenic temperature, some of these pollutions lead to a strong decrease of the material ductility. In order to validate the Ti6Al4V powder metallurgy route for critical engine components, it is necessary to understand and quantify the influence of such pollutions. Due to diffusion during the compaction cycle, several layers with different chemical and crystallographic properties are formed. In this paper, an analysis by SEM and TEM of these phases is presented. Moreover, mechanical tests at 20K, including interrupted tensile tests, allow to discriminate the worst potential defects and to propose several fracture processes depending on the initial impurity chemical composition. KEYWORDS Ti6Al4V, powder metallurgy, defects, fracture mechanisms INTRODUCTION The improvement of rocket engine efficiency necessitates components with an increasing complex geometry. For cryogenic applications, the α/β Ti6Al4V titanium alloy is used owing to its high strength, specific modulus and ductility at such temperatures. To achieve complex geometry, the powder metallurgy route is foreseen with the additional advantage that it provides a good homogeneity of the microstructure. However, a major drawback comes from the possible presence of impurities in the initial powder before compaction. These impurities can be introduced either during the melting operation, during powder production or during subsequent handling. Some defects can be quite large, typically 500 µm diameter including the diffusion affected volume, and lead to a strong decrease of the ductility of the material at low temperature (20K) under monotonic loading. The aim of this study is to investigate the effect of various defects on the ductility as well as to understand the failure mechanisms in order to predict the rupture of a component under in-service conditions.

RkJQdWJsaXNoZXIy MjM0NDE=