ICF10B

POSTER REFERENCE: ICF100568OR CORROSION AND STRENGTH DEGRADATION OF Si-BASED CERAMICS BY MOLTEN SALT NAOYA MASUDA1 and YUJI KIMURA2 1Graduate Student, Kogakuin Univ.1-24-2 Nishishinjuku,Shinjuku-ku,Tokyo,163-8677, Japan 2Department of Material Science and Technology, Kogakuin Univ.1-24-2 Nishishinjuku,Shinjuku-ku,Tokyo,163-8677, Japan ABSTRACT Several trials have been conducted for applying Si-based ceramics as the materials used for the high temperature structure such as gas turbine components, because of there superior fracture toughness and thermal shock resistance under high temperature condition. However, various problems concerning oxidation and corrosion under high temperature environment have been reported. From among various high temperature corrosion problems, the molten salt corrosion has been pointed out as the most important one which caused serious fracture strength degradation. Purpose of this study is to evaluate the corrosion behavior and the degradation in the mechanical property of SiC and Si3N4 caused by molten salt. As a result, the influence of molten salt Na2SO4 upon the mechanical property of structural ceramics SiC and Si3N4 was made clear to be caused by the progressive corrosion reaction, i.e. the successive repetition of the generation and removal of the SiO2 membrane under the high temperature condition. KEYWORDS: SiC, Si3N4, gas turbine, molten salt Na2SO4, corrosion, oxidation, SiO2, strength degradation, INTRODUCTION The application of Si-based ceramics is expected as the material of the high temperature structure such as gas turbine etc. because SiC and Si3N4 have excellent fracture strength, fracture toughness and thermal shock resistance under high temperature condition. It was pointed out that the materials used for the high temperature

RkJQdWJsaXNoZXIy MjM0NDE=