Figure 6: Relation Between Defect Area and Strength CONCLUSIONS Corrosion characteristics and degradation in the mechanical properties of Si-based structural ceramics such as SiC and Si3N4 by molten salt of Na2SO4 were investigated. Results obtained are summarized as follows: 1. The influence of molten salt Na2SO4 upon the mechanical property of structural ceramics SiC and Si3N4 was made clear to be caused by the progressive corrosion reaction, i.e. the successive repetition of the generation and removal of the SiO2 membrane under the high temperature condition. 2. Also, the degradation of the mechanical property by the progress of the molten salt corrosion under high temperature environment became clear to be saturated within 0.5 hours. 3. Furthermore, the residual bending strength after molten salt corrosion can be investigated on the basis of fracture mechanics view point. In case of Si3N4 ceramics, KIC can be evaluated on the basis of square root depth of babble formed layer. On the other hand, in case of SiC ceramics, it can be evaluated based on fracture origin defect area. Accordingly, it is required to pay sufficient attentions to the existence of the molten salt when Si-baced ceramics such as SiC and Si3N4 are used under the high temperature environment. REFERENCES 1. T Sato, Y Koike, T Endo, M Shimada, (1988) J. Soc. Mat. Sci., Japan, Vol.38, No.424, 39-43 2. JIS R 1601, (1994) Testing method for flexural strength of high performance ceramics 3. Nathan S. Jacobson, (1993) J. Am. Ceram. Soc., 76(1)3-28 4. Catalog of Sintered SiC “CERASIC B”, Toshibaceramics Co. Ltd. 5. Catalog of Gasometrical sintering Si3N4, NTK Co. Ltd. 6. Y Murakami, S Nemat-Nasser, (1983) Engineering Fracture Mechanics, Vol.17, No.3, 193-210

RkJQdWJsaXNoZXIy MjM0NDE=