ICF10B

CONCLUSION The time life and the crack propagation rate minimum can be explained from a power law of the hole radius. The cold expansion bring a advantageous effect until a limit value, over this value the expansion is damaging. The advantageous effect can be explained in the same way that the hole radius effect. The time life versus the stress amplitude leads to similar curves that Wöhler curves and they can be used in the same way. The residual compressive stresses and the plastic zone size was calculated from three dimensions F.E.M. Alone Theses parameters can’t explain the material behaviour . The local microstructure modifications must have a great part in the new crack initiation. The crack tip opening displacement can be used as a picture of the hole radius, of the cold expansion and of the residual stresses distribution. BIBLIOGRAPHY [1] Domazet Z, (1996) Engenering Failure Analysis, , 3 (2): 137-147 [2] R.Ghfiri, A. Amrouche, A.Imad, G. Mesmacque (2000) International journal of fatigue and Fracture Engineering Materials and Structures Vol 23 pp911-916 [3] Landy.M.L, Armen.H.J, Eidinoff .H.L.(1986). Fatigue in Mechanically Fastened Composite and Metallic Joints. ASTM STP 927 pp 190-220. [4] Bernard M, Bui-Quoc T. and Burlat M., Fatigue. Fract. Engng. Mater. Struct, (1995), No 18, pp765-775. [5] Baker A.A., (1993), Fatigue. Fract. Engng. Mater. Struct.No 16, pp753-765. [6].Cathey W.H and .Grandt A.F, (1980), J. Engng. Mat. Tech, No 102, pp 85-91.

RkJQdWJsaXNoZXIy MjM0NDE=