ORAL REFERENCE: ICF100160OR EFFECT OF PREDEFORMATION ON FATIGUE LIFE – EXPERIMENTAL CHARACTERIZATION AND DESCRIPTION BY MEANS OF A NEW PARAMETER H.-J. Christ and K. Schoeler Institut für Werkstofftechnik, Universität Siegen, D-57068 Siegen, Germany ABSTRACT Isothermal cyclic deformation tests were carried out on two nickel-base alloys (Nimonic 105 and Nimonic 75) after monotonic predeformation to various strains. The test temperatures ranged from room temperature up to 800°C, and plastic strain amplitudes between 0.025% and 0.25% were applied. The effect of predeformation was found to lose importance with increasing temperature, increasing plastic strain amplitude, decreasing prestrain and decreasing influence of particle strengthening. Appreciable changes in the crack initiation process and the dislocation arrangement resulted from predeformation. However, the change in the cyclic stress-strain response was identified to be the main reason for the effect of predeformation on fatigue life. Consequently, a new parameter SP_SWT was derived which is based on the values of the Smith-Watson-Topper damage parameter obtained in fatigue tests on predeformed and not predeformed samples, respectively. It was shown that SP_SWT is suitable to quantitatively describe the effect of loading conditions on the prehistory dependence and can successfully be applied for a simple and temperature-independent prediction of the influence of a predeformation on fatigue lifetime. KEYWORDS Predeformation, prehistory dependence, nickel-base alloys, cyclic stress-strain behaviour, microstructure, fatigue lifetime, damage parameter, high temperature INTRODUCTION Microstructure-related and mechanism-oriented studies on the cyclic deformation behaviour of metals and alloys mostly deal with materials in well-defined annealed starting conditions, in order to obtain results that are both definite and reproducible. Consequently, from all the parameters which are known to strongly influence cyclic stress-strain response and fatigue lifetime, such as loading amplitude, temperature and testing mode, least is know about the parameter mechanical prehistory. However, almost all engineering materials used in structural applications undergo a (thermo-)mechanical pre-treatment, either during the fabrication process or as a means to optimise the mechanical properties. Hence, the prehistory dependence of the cyclic deformation behaviour is on the one hand of high technical significance and on the other hand a complex scientific challenge. Earlier studies which were focussing on single-phase fcc metals and alloys indicated the important role of the dislocation slip character [1-3]. In the case of planar slip, even a small monotonic prestrain gives rise to
RkJQdWJsaXNoZXIy MjM0NDE=