3.2.2 Alumina polished specimen Additional potentiodynamic polarization tests were carried out for the alumina polished specimen. Fig.8 shows the polarization curves, together with the results for the ELID ground specimens. This result indicates that the corrosion property of the #8000 series is more superior than that of the alumina polished specimen. Besides, the value of the surface roughness on the ELID ground specimen is the same as that on the alumina polished specimen. 4. DISCUSSION Table2 summarizes the values of Ecorr, Epit and Ipass observed from the potentiodynamic polarization tests (Fig.6 and Fig.8). Remarkable differences in the values between the #8000 series and the alumina series are observed. To clarify the reason for this, a surface analysis was performed by using SEM and EDX. Fig.9 shows the results. The ELID ground sample had a high value of carbon and oxygen. This implies that the surface of the ELID ground sample was covered with some kind of oxide film ; existence of the film leads to an excellent corrosion property on the ELID ground specimen. With ELID grinding, in the small clearance between the two poles, electrolysis occurs upon supply of a chemically soluble grinding fluid and an electrical current. It could be suggested that chemical reactions between oxygen and the heated specimen, due to the ELID grinding, results in the existence of oxide film. Table2 Polarization test results on surface finished stainless steel Fig.8 Anodic polarization curves of stainless steel for the specimen with different surface finishings 3.32 310 -131 alumina series 0.86 427 43 #8000 series 2.00 330 -23 #2000 series - 52 -142 #325 series Ipass (10-4 mA/cm2) Epit (mV vs S.C.E) Ecorr (mV vs S.C.E) Potential (V vs S.C.E) Current density (mA/cm2) -0.2 -0.1 0 0.1 0.2 0.3 0.4 0.5 101 100 10-1 10-2 10-3 10-4 10-5 10-6 (3) (4) (3) alumina series (4) #8000 series
RkJQdWJsaXNoZXIy MjM0NDE=